Preparation method of anti-bacterial deodorant leather
A technology for leather and leather materials, which is applied in the field of antibacterial and deodorizing leather preparation, which can solve the problems of poor air permeability, bacteria and fungi breeding, etc., and achieve the effect of eliminating peculiar smell and excellent antibacterial and deodorizing effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0024] The invention provides a kind of preparation method of antibacterial deodorization leather, comprises the following steps:
[0025] (1) After degreasing and neutralizing the wet blue leather successively, a neutral base material is obtained;
[0026] (2) rotating and mixing the neutral base material obtained in the step (1) with ammonia, dyestuffs and micron silver powder in a drum to obtain dyed leather;
[0027] (3) carrying out fatliquoring and acid-fixing treatment successively to the dyed leather obtained in the step (2) to obtain primary leather;
[0028] (4) The primary leather obtained in the step (3), water, deodorant resin mixture, anionic deodorant, cross-linking agent, silicone softener and formic acid are rotated and mixed in a drum to obtain an antibacterial deodorant Leather; the deodorant resin mix contains fragrance and resin nanoparticles.
[0029] In the present invention, unless otherwise specified, the materials used in the preparation process are...
Embodiment 1
[0048] Weighing: Weigh the raw material wet blue hide, and take the weight of the wet blue hide as 100wt.%. The mass involved in the subsequent steps is based on this.
[0049] Degreasing: Put the wet blue hide into the drum, add 45°C water, degreasing agent and formic acid, and then rotate for 60 minutes, then wash with water to remove the residual formic acid and degreasing agent on the surface of the wet blue hide; Liquid removal; Wherein, the wet blue leather mass taken by weighing is 100wt.%, the addition of water is 100wt.%, the addition of degreasing agent is 0.5wt.%, and the addition of formic acid is 0.2wt.%.
[0050] Neutralization: At room temperature, add 100wt.% water at 30°C to the drum that retains the degreased wet-blue leather, then add 3% baking soda and 3% ammonium bicarbonate and continue to rotate for 90 minutes. Measure the pH value of the liquid in the drum at 6.5; finally wash with water, and remove the liquid in the drum after washing.
[0051] Dyeing...
Embodiment 2
[0057] Prepare antibacterial and deodorant leather according to the method of Example 1, the difference is that in the dyeing process, the particle size of the micron silver powder is 3 μm, and the dosage is 0.2%; 1:2 mixture of essence and polypropylene resin nanoparticles (particle size less than 1μm), anionic ion deodorant is nano-scale ferrous chloride, cross-linking agent is methacrylic acid, silicone softener is containing dioxide Fatty alcohol sulfate derivatives of silicon; and the amount of the deodorant resin mixture is 0.05%, and the amount of the anionic deodorant is 2.0%.
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com