[0031] A waterproof paper pulp additive, comprising the following raw materials in parts by weight: 25 parts of candelilla wax, 2 parts of dipotassium glycyrrhizinate, 10 parts of polyvinyl alcohol, 1 part of polyvinyl butyral, methylated amino 2 parts of resin, 22 parts of tetrapod zinc oxide whiskers, 54 parts of liquid paraffin, 22 parts of polydimethylsiloxane, 1 part of aqueous zinc stearate, 2 parts of hydroxypropyl cellulose, 3 parts of guanidine carbonate, 1 part of potassium pyrophosphate, 10 parts of guanidine phosphate and 1 part of butyl titanate.
[0032] A kind of preparation method of waterproof pulp auxiliary agent comprises the following steps:
[0033] 1) Pour 25 parts of candelilla wax into a pulverizer for pulverization, pulverize the candelilla wax into 0.1 μm, and prepare candelilla wax powder for later use;
[0034] 2) Mix 2 parts of dipotassium glycyrrhizinate, 10 parts of polyvinyl alcohol, 1 part of polyvinyl butyral, 2 parts of methylated amino resi...
Embodiment 2
[0036] A waterproof pulp additive, comprising the following raw materials in parts by weight: 33 parts of candelilla wax, 4 parts of dipotassium glycyrrhizinate, 14 parts of polyvinyl alcohol, 3 parts of polyvinyl butyral, methylated amino 4 parts of resin, 24 parts of tetrapod zinc oxide whiskers, 78 parts of liquid paraffin, 41 parts of polydimethylsiloxane, 3 parts of aqueous zinc stearate, 4 parts of hydroxypropyl cellulose, 4 parts of guanidine carbonate, 3 parts of potassium pyrophosphate, 13 parts of guanidine phosphate and 4 parts of butyl titanate.
[0037] A preparation method of waterproof pulp additive, comprising the following steps:
[0038] 1) Pour 33 parts of candelilla wax into a pulverizer for pulverization, pulverize the candelilla wax into 0.3 μm, and prepare candelilla wax powder for later use;
[0039] 2) Mix 4 parts of dipotassium glycyrrhizinate, 14 parts of polyvinyl alcohol, 3 parts of polyvinyl butyral, 4 parts of methyl etherified amino resin, 24 p...
Embodiment 3
[0041] A waterproof paper pulp additive, comprising the following raw materials in parts by weight: 30 parts of candelilla wax, 3 parts of dipotassium glycyrrhizinate, 12 parts of polyvinyl alcohol, 2 parts of polyvinyl butyral, methylated amino 3 parts of resin, 23 parts of tetraacicular zinc oxide whiskers, 60 parts of liquid paraffin, 30 parts of polydimethylsiloxane, 2 parts of aqueous zinc stearate, 3 parts of hydroxypropyl cellulose, 4 parts of guanidine carbonate, 2 parts of potassium pyrophosphate, 12 parts of guanidine phosphate and 3 parts of butyl titanate.
[0042] A preparation method of waterproof pulp additive, comprising the following steps:
[0043] 1) Pour 30 parts of candelilla wax into a pulverizer for pulverization, and pulverize the candelilla wax into 0.2 μm to obtain candelilla wax powder for later use;
[0044] 2) Mix 3 parts of dipotassium glycyrrhizinate, 12 parts of polyvinyl alcohol, 2 parts of polyvinyl butyral, 3 parts of methyl etherified amino...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com