[0013] The invention provides a method for preparing a moisture-proof cable sheath, comprising:
[0014] 1) ultrasonically vibrate the molecular sieve, graphene, porous starch and water, and then dry to prepare the mixture;
[0015] 2) Soak the mixture, nano-zinc dioxide, and nano-tin dioxide, and then filter to obtain a moisture-proof additive;
[0016] 3) Mixing and molding natural rubber, polyvinyl chloride, dioctyl terephthalate, hydroxymethyl starch, bentonite, nano-titanium dioxide, silicone oil, sulfur and moisture-proof additives to obtain a moisture-proof cable sheath.
[0017] In step 1) of the present invention, the consumption of each material can be selected in a wide range, but in order to further improve the moisture-proof performance of cable sheath, preferably, in step 1), molecular sieve, graphene, porous starch and water The weight ratio is 50:10-15:18-22:150-250.
[0018] In step 1) of the present invention, the condition of ultrasonic vibration can be se...
Embodiment 1
[0027] 1) Ultrasonic vibration of molecular sieve, graphene, porous starch and water according to the weight ratio of 50:13:20:200 (ultrasonic frequency is 28KHz, vibration time is 50min), and then dried (drying temperature is 110°C, drying time is 3h) to produce a mixture;
[0028] 2) Soak the mixture, nano-zinc dioxide, and nano-tin dioxide in a weight ratio of 100:4:2.5 (soaking temperature is 40° C., soaking time is 13 hours), and then filtered to obtain moisture-proof additive A1.
Embodiment 2
[0030] 1) Ultrasonic vibration of molecular sieve, graphene, porous starch and water according to the weight ratio of 50:10:18:150 (ultrasonic frequency is 25KHz, vibration time is 60min), and then dried (drying temperature is 100°C, drying time is 4h) to produce a mixture;
[0031] 2) Soak the mixture, nano-zinc dioxide, and nano-tin dioxide in a weight ratio of 100:3:1.5 (the soaking temperature is 35° C., and the soaking time is 16 hours), and then filter to obtain the moisture-proof additive A2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com