Wood softener, and preparation method and application thereof

A kind of softener and wood technology, which is applied in wood treatment, impregnated wood, wood impregnation, etc., can solve the problems that wood cannot be accurately identified, consumer rights cannot be guaranteed, and softening efficiency needs to be improved, so as to achieve good softening effect and reduce High softening time and softening efficiency

Active Publication Date: 2019-02-22
派韵家具江苏有限公司
View PDF8 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Wood has a wide range of functions, mainly used in construction and daily necessities. When manufacturing these products, wood needs to be processed accordingly. The processed wood cannot be accurately identified, and merchants may mislead consumers, so that consumer rights cannot be guaranteed. , so it is necessary to identify the slice softening of wood
[0003] Traditional wood softening is mainly cooking in boiling water, which takes several weeks to soften, high energy consumption, and low softening efficiency. In order to improve softening efficiency and reduce softening costs, wood softeners are mainly used to accelerate softening, but the current wood softeners are mainly softening. The aqueous solution of the agent usually needs to be softened at high temperature for half a day to one day, and the softening efficiency needs to be improved

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Wood softener, and preparation method and application thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0019] A wood softener, comprising the following raw materials in parts by weight: 14 parts of hydrogen peroxide, 5 parts of oleoylethanolamine, 4 parts of potassium trifluoromethanesulfonate, 2 parts of N,N-dimethylacetamide, 1 part of lithium acetate, Sodium tripolyphosphate 0.8 part.

[0020] A preparation method of wood softener, comprising the following steps:

[0021] (1) Heat the hydrogen peroxide to 45°C, add lithium acetate and sodium tripolyphosphate and stir for 20 minutes under the stirring condition of 300rpm;

[0022] (2) Raise the temperature in step (1) to 60°C, add oleoylethanolamine and continue stirring for 10 minutes;

[0023] (3) Reduce the temperature in step (2) to 20°C, add potassium trifluoromethanesulfonate and N,N-dimethylacetamide, and stir evenly to obtain a wood softener.

Embodiment 2

[0025] A wood softener, comprising the following raw materials in parts by weight: 15 parts of hydrogen peroxide, 5.5 parts of oleoylethanolamine, 4.5 parts of potassium trifluoromethanesulfonate, 2.5 parts of N,N-dimethylacetamide, 2 parts of lithium acetate, 0.9 parts of sodium tripolyphosphate.

[0026] A preparation method of wood softener, comprising the following steps:

[0027] (1) Heat the hydrogen peroxide to 48°C, add lithium acetate and sodium tripolyphosphate under stirring condition of 350rpm and stir for 25min;

[0028] (2) Raise the temperature in step (1) to 60°C, add oleoylethanolamine and continue stirring for 12 minutes;

[0029] (3) Reduce the temperature in step (2) to 22°C, add potassium trifluoromethanesulfonate and N,N-dimethylacetamide and stir evenly to obtain a wood softener.

Embodiment 3

[0031] A wood softener, comprising the following raw materials in parts by weight: 16 parts of hydrogen peroxide, 6 parts of oleoylethanolamine, 5 parts of potassium trifluoromethanesulfonate, 3 parts of N,N-dimethylacetamide, 3 parts of lithium acetate, Sodium tripolyphosphate 1 part.

[0032] A preparation method of wood softener, comprising the following steps:

[0033] (1) Heat the hydrogen peroxide to 50°C, add lithium acetate and sodium tripolyphosphate and stir for 30 minutes under the stirring condition of 400rpm;

[0034] (2) Raise the temperature in step (1) to 60°C, add oleoylethanolamine and continue stirring for 15 minutes;

[0035] (3) Reduce the temperature in step (2) to 25°C, add potassium trifluoromethanesulfonate and N,N-dimethylacetamide and stir evenly to obtain a wood softener.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a wood softener, and a preparation method and application thereof. The wood softener is composed of the following materials, by weight: 14-18 parts of hydrogen peroxide, 5-7 parts of oleoyl cholamine, 4-6 parts of potassium trifluoromethane sulfonate, 2-4 parts of N,N-Dimethylacetamide, 1-5 parts of lithium acetate, and 0.8-1.2 parts of sodium tripolyphosphate, The wood sofener is prepared from hydrogen peroxide, oleoyl ethanolamine, trifluoromethane sulfonic acid potassium, N,N-Dimethyl acetamide, and lithium acetate and sodium tripolyphosphate according to the process; the prepared wood softener has low softening temperature and short softening time; under the same softening temperature, the softening time can be shortened by about 50%; softening efficiency is high, the cost of the wood softening can be reduced, and the softening effect is good; and the preparation method is simple, can easily achieve industrial production and is worth popularizing.

Description

technical field [0001] The invention relates to a chemical auxiliary agent, in particular to a wood softener and its preparation method and application. Background technique [0002] Chemical additives are chemical additives used in a certain industry. There are many types, generally including metal processing additives, plastic additives, papermaking additives, construction additives, water treatment additives, coating additives, leather additives , Auxiliaries for the electronics industry, textile printing and dyeing auxiliaries, wood auxiliaries, etc. Wood has a wide range of functions, mainly used in construction and daily necessities. When manufacturing these products, wood needs to be processed accordingly. The processed wood cannot be accurately identified, and merchants may mislead consumers, so that consumer rights cannot be guaranteed. , so it is necessary to identify the slice softening of wood. [0003] Traditional wood softening is mainly cooking in boiling wa...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): B27K5/06B27K3/52
CPCB27K3/52B27K5/06
Inventor 杨迪忠
Owner 派韵家具江苏有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products