A moisturizing agent and tobacco technology, applied in the field of tobacco, can solve the problems of producing peculiar smell, unfavorable to the taste and aroma of tobacco, etc., and achieve the effects of prolonging durability, excellent moisturizing and aroma-fixing dual functions, and strong operability.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] A tobacco aroma-fixing moisturizer, which comprises the following components in parts by weight of raw materials:
[0021]
[0022]
[0023] Preparation:
[0024] 1) Mix the mixture of propylene glycol and glycerin with the alcohol-soluble naringin extract in parts by weight of raw materials, heat up to 50° C., and stir at 1200 rpm for 20 minutes to obtain an alcohol mixture;
[0025] 2) Mix the water-soluble Luo Han Guo powder and distilled water in parts by weight of raw materials, heat up to 50° C., and stir at 1200 rpm for 20 minutes to obtain a water-soluble mixture;
[0026] 3) Mix the alcohol mixture obtained in step 1) with the water-soluble mixture described in step 2), add the Maillard reactant, stir at 1200 rpm for 40 minutes, and obtain the finished product of Example 1.
Embodiment 2
[0028] A tobacco aroma-fixing moisturizer, which comprises the following components in parts by weight of raw materials:
[0029]
[0030] Preparation:
[0031] 1) Mix the mixture of glycerol and sorbitol with the alcohol-soluble pomelo polysaccharide in parts by weight of raw materials, heat up to 70°C, and stir at 800rpm for 30min to obtain the alcohol mixture;
[0032] 2) Mix water-soluble steviol glycosides and distilled water in parts by weight of raw materials, heat up to 70°C, and stir at 800 rpm for 30 minutes to obtain a water-soluble mixture;
[0033] 3) Mix the alcohol mixture obtained in step 1) with the water-soluble mixture described in step 2), add the Maillard reactant, stir at 800 rpm for 20 minutes, and obtain the finished product of Example 2.
Embodiment 3
[0035] A tobacco aroma-fixing moisturizer, which comprises the following components in parts by weight of raw materials:
[0036]
[0037] Preparation:
[0038] 1) Mix the mixture of propylene glycol, glycerin and sorbitol with the alcohol-soluble neomethylhesperidin extract in parts by weight of raw materials, heat up to 60°C, and stir at 1000rpm for 25min to obtain the alcohol mixture;
[0039] 2) Mix the water-soluble Luo Han Guo extract and distilled water in parts by weight of raw materials, heat up to 60° C., and stir at 1000 rpm for 25 minutes to obtain a water-soluble mixture;
[0040] 3) Mix the alcohol mixture obtained in step 1) with the water-soluble mixture described in step 2), add the Maillard reactant, stir at 1000 rpm for 30 minutes, and obtain the finished product of Example 3.