Treatment method for improving dyeing stability of wood
A treatment method and a stable technology, applied in wood treatment, wood heat treatment, pressurized wood treatment, etc., can solve the problems of affecting quality and life, poor coloring effect, etc., and achieve strong fixing ability, good promotion and use value, The effect of improving the fixation ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] A treatment method for improving the staining stability of wood, comprising the steps of:
[0040] (1) Steam explosion treatment:
[0041] Put the wood into the steam explosion tank, and then introduce high-temperature water vapor with a temperature of 102°C into the steam explosion tank, and increase the pressure in the steam explosion tank to 0.35MPa. Unload the steam explosion tank to normal temperature and pressure, and take it out for later use;
[0042] (2) Surface treatment liquid spraying treatment:
[0043] Spray the pre-prepared surface treatment solution evenly on the wood surface treated in step (1), and use it for later use; the surface treatment solution is specifically composed of the following substances in corresponding parts by weight: 10 parts of enhanced attapulgite , 5 parts of sodium hexametaphosphate, 2 parts of calcium stearate, 3 parts of nonylphenol polyoxyethylene ether, 180 parts of deionized water;
[0044] (3) Grinding treatment:
[004...
Embodiment 2
[0050] A treatment method for improving the staining stability of wood, comprising the steps of:
[0051] (1) Steam explosion treatment:
[0052] Put the wood into the steam explosion tank, and then introduce high-temperature water vapor at a temperature of 105°C into the steam explosion tank, and increase the pressure in the steam explosion tank to 0.4MPa, heat preservation and pressure treatment for 120s, and then in 20s Unload the steam explosion tank to normal temperature and pressure, and take it out for later use;
[0053] (2) Surface treatment liquid spraying treatment:
[0054]Spray the pre-prepared surface treatment liquid evenly on the wood surface treated in step (1), and use it for later use; the surface treatment liquid is specifically composed of the following substances in corresponding parts by weight: 15 parts of enhanced attapulgite , 8 parts of sodium hexametaphosphate, 4 parts of calcium stearate, 5 parts of nonylphenol polyoxyethylene ether, 200 parts of...
Embodiment 3
[0061] A treatment method for improving the staining stability of wood, comprising the steps of:
[0062] (1) Steam explosion treatment:
[0063] Put the wood into the steam explosion tank, and then introduce high-temperature water vapor with a temperature of 104°C into the steam explosion tank, and increase the pressure in the steam explosion tank to 0.38MPa. Unload the steam explosion tank to normal temperature and pressure, and take it out for later use;
[0064] (2) Surface treatment liquid spraying treatment:
[0065] Spray the pre-prepared surface treatment solution evenly on the wood surface treated in step (1), and use it for later use; the surface treatment solution is specifically composed of the following substances in corresponding parts by weight: 13 parts of enhanced attapulgite , 7 parts of sodium hexametaphosphate, 3 parts of calcium stearate, 4 parts of nonylphenol polyoxyethylene ether, 190 parts of deionized water;
[0066] (3) Grinding treatment:
[006...