Preparation method, applications and regeneration methods of chitosan-modified zeolite molecular sieve
A zeolite molecular sieve and chitosan modification technology, applied in the field of molecular sieves, can solve problems such as health hazards of residents, and achieve the effects of lively properties, improved mechanical properties, and excellent effects.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0042] A kind of preparation method of chitosan modified zeolite molecular sieve of the present embodiment comprises the following steps:
[0043] a. Wash the zeolite molecular sieve with deionized water, put it into an oven, and dry it at 103°C for 1.5h;
[0044] B, the chitosan of 7.5g / L is dissolved in the acetic acid solution of 4.5vol%, is configured into chitosan acetic acid sol;
[0045] c. Weigh the dried zeolite molecular sieve and put it into the chitosan acetate gel in step b, and then place it in a constant temperature oscillator with a rotation speed of 130r / min. Under the condition of an oscillation temperature of 28°C, the oscillation time is 8h, and the process is completed. Combination of chitosan acetic acid sol and zeolite molecular sieve;
[0046] d. Take out the combined particles, rinse them with deionized water until they are neutral, then place them in an oven, and dry them for 11 hours at a temperature of 55°C.
Embodiment 2
[0048]A kind of preparation method of chitosan modified zeolite molecular sieve of the present embodiment comprises the following steps:
[0049] a. Wash the zeolite molecular sieve with deionized water, put it in an oven, and dry it at 107°C for 2.5h;
[0050] B, the chitosan of 8.5g / L is dissolved in the acetic acid solution of 5.5vol%, is configured into chitosan acetic acid sol;
[0051] c. Weigh the dried zeolite molecular sieve and put it into the chitosan acetate gel in step b, and then place it in a constant temperature oscillator with a rotation speed of 150r / min. Under the condition of an oscillation temperature of 32°C, the oscillation time is 12h, and the process is completed. Combination of chitosan acetic acid sol and zeolite molecular sieve;
[0052] d. Take out the combined particles, rinse them with deionized water until neutral, then place them in an oven, and dry them for 13 hours at a temperature of 65°C.
Embodiment 3
[0054] A kind of preparation method of chitosan modified zeolite molecular sieve of the present embodiment comprises the following steps:
[0055] a. Wash the zeolite molecular sieve with deionized water, put it in an oven, and dry it at 105°C for 2 hours;
[0056] B, dissolving the chitosan of 8g / L in the acetic acid solution of 4vol%, is configured to be configured into chitosan acetic acid sol;
[0057] c. Weigh the dried zeolite molecular sieve and put it into the chitosan acetate gel in step b, and then place it in a constant temperature oscillator with a rotation speed of 140r / min. Under the condition of an oscillation temperature of 30°C, the oscillation time is 10h, and the process is completed. Combination of chitosan acetic acid sol and zeolite molecular sieve;
[0058] d. Take out the combined particles, wash them with deionized water until they are neutral, then place them in an oven, and dry them for 12 hours at a temperature of 60°C.
[0059] For the performanc...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
adsorption capacity | aaaaa | aaaaa |
clearance rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com