Method for treating potassium ammonium group drilling fluid rock debris
A treatment method and drilling fluid technology, which can be used in earth-moving drilling, flushing wellbore, wellbore/well components, etc., and can solve the problems of large dosage, excessive COD, and high pH.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] Add silicon micropowder, aluminum salt and iron salt with a mass ratio of 1:5:2 in sequence and stir and mix for 3 minutes at a speed of 150 rpm to obtain a rock debris breaker.
Embodiment 2
[0037] Add silicon micropowder, aluminum salt and iron salt with a mass ratio of 4:15:2 in sequence, and stir and mix at a speed of 250 rpm for 3 minutes to obtain a rock debris breaker.
Embodiment 3
[0039] Sequentially add silicon micropowder, aluminum salt and iron salt with a mass ratio of 1:12:5 and stir and mix for 4 minutes at a speed of 200 rpm to obtain a rock debris breaker.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com