Method for reducing irritation of papermaking-process tobacco sheets

A tobacco flake and irritating technology, which is applied in the field of paper-making tobacco flake preparation, can solve the problems of ineffectiveness, protection, and loss of flavor substances, and achieve the effects of reducing irritation, good sensory quality, and inhibiting volatilization

Active Publication Date: 2021-03-05
山东瑞博斯烟草有限公司
View PDF11 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Although this method reduces the irritation, the high-temperature drying process of tobacco flakes causes a large loss of the arom

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Method for reducing irritation of papermaking-process tobacco sheets
  • Method for reducing irritation of papermaking-process tobacco sheets

Examples

Experimental program
Comparison scheme
Effect test

preparation example Construction

[0026] A method for reducing the irritation of paper-making tobacco sheets, said preparation method comprising the steps of:

[0027] Step A, preparation of tobacco powder ethanol extract: use ethanol to extract tobacco powder, separate and obtain ethanol extract, and concentrate ethanol extract to obtain alcohol-soluble concentrate;

[0028] Step B, preparation of alcohol-soluble coating solution: add a certain amount of other plant alcohol-soluble extracts, glycerin, Amadori compound, monoglyceride, sweetener, etc. to the above-mentioned alcohol-soluble concentrate to prepare alcohol-soluble coating solution ;

[0029] Step C, carrier solution preparation: prepare a certain concentration of β-cyclodextrin solution;

[0030] Step D: Preparation of the carrier-based alcohol-soluble coating solution: adding a certain proportion of the alcohol-soluble coating solution to the carrier-based solution and mixing fully;

[0031] Step E: Preparation of carrier-based alcohol-soluble ...

Embodiment 1

[0053] A, the preparation of tobacco powder ethanol extract: take a certain amount of tobacco powder, add 10 times the quality of ethanol, stir and extract at 60°C for 1h, centrifuge to obtain the ethanol extract and residue, and concentrate the ethanol extract (concentrate to 1 / 15 of the original volume), to obtain the alcohol-soluble concentrate;

[0054] B, preparation of alcohol-soluble coating solution: add 20% Aiye Alcohol-soluble extract, 5% glycerol, 5% Amadori compound, 1% monoglyceride, 1% glucose to the above-mentioned alcohol-soluble concentrate, Preparation of alcohol-soluble coating solution;

[0055] C. Carrier solution preparation: configure a β-cyclodextrin solution with a mass concentration of 15%;

[0056] D. Preparation of carrier-based alcohol-soluble coating solution: add 10% alcohol-soluble coating solution to the β-cyclodextrin solution, and mix well;

[0057] E. Preparation of carrier-based alcohol-soluble coating solution: add 2% prolamin into step ...

Embodiment 2

[0060] A, the preparation of tobacco powder ethanol extract: take a certain amount of tobacco powder, add 10 times the quality of ethanol, stir and extract at 60°C for 1h, centrifuge to obtain the ethanol extract and residue, and concentrate the ethanol extract (concentrate to 1 / 15 of the original volume), to obtain the alcohol-soluble concentrate;

[0061] B. Carrier solution preparation: prepare a β-cyclodextrin solution with a mass concentration of 15%;

[0062] C. Preparation of carrier-based alcohol-soluble coating solution: add the 10% alcohol-soluble coating solution obtained in step A into the β-cyclodextrin solution, and mix well;

[0063] D. Preparation of carrier-based alcohol-soluble coating solution: add 2% prolamin to step C, and mix well;

[0064] E. Preparation of tobacco sheet: Add the carrier-based alcohol-soluble coating solution in the above step D to the coating solution obtained in step A in comparative example 1 at a ratio of 5%, and prepare tobacco she...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to a method for reducing irritation of paper-making tobacco sheets, and belongs to the field of paper-making tobacco sheet preparation. The method comprises the following steps:carrying out alcohol extraction and concentration on tobacco powder to obtain an alcohol-soluble concentrate; uniformly mixing the alcohol-soluble concentrate with an alcohol-soluble extract of a plant, glycerol, an Amadori compound, monoglyceride and a sweetening agent to obtain an alcohol-soluble coating solution; uniformly mixing the alcohol-soluble coating solution with a carrier solution, adding alcohol-soluble protein, and uniformly mixing to obtain a carrier alcohol-soluble coating liquid; adding the carrier alcohol-soluble coating liquid into a conventional tobacco sheet coating liquidto prepare a coating liquid; and adding the coating liquid into a tobacco sheet paper base, and drying to obtain the tobacco sheet. Although the content of harmful components such as tar is low, thecontent of carbon monoxide is high, the drying feeling is serious, irritation is large, smoke is not coordinated, and wood gas is serious in an existing tobacco sheet, so irritation of the papermakingmethod tobacco sheet is reduced.

Description

technical field [0001] The invention belongs to the technical field of paper-making tobacco sheet preparation, and in particular relates to a method for reducing the irritation of paper-making tobacco sheet. Background technique [0002] The information disclosed in this background section is only intended to increase the understanding of the general background of the present invention, and is not necessarily taken as an acknowledgment or any form of suggestion that the information constitutes the prior art already known to those skilled in the art. [0003] Tobacco sheet is a product that is recombined by using waste from the production process of cigarettes such as tobacco stems, tobacco powder, and shredded tobacco sheets, plus plant fibers, and is also called reconstituted tobacco leaves. At the beginning of its development, it was to save raw materials and reduce costs. The development of tobacco sheet has gone through three stages: roll pressing method, thick pulp met...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): A24B3/14A24B3/12
CPCA24B3/14A24B3/12
Inventor 邢振雷迟建国徐利高颖田海龙张家树李刚李玲李晓华
Owner 山东瑞博斯烟草有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products