[0020] A manufacturing process of low-cost artificial travertine, comprising the following steps carried out in sequence: a. granulation, selecting one or more mixed commercially available slow-dissolving substances, slow-dissolving substances including A substance, B substance and C substance , preferably the A substance: B substance: C substance = 20:30:3. The substance A is a water-soluble powder, and the substance A is ammonium bicarbonate or urea. The substance B is a water-soluble powder, and the substance B is polyacrylamide. The substance C can be dissolved into a liquid only under acidic or alkaline conditions. The substance C is an alkali-soluble acrylic resin or a low-temperature acid-soluble resin at 45-55° C., and its main function is to wrap soluble particles. Substance C contains water, and this part of water can dissolve 23-27% of Substance A and / or Substance B. Mix uniformly according to the weight ratio of the total amount of slow-dissolving substances and ...
Embodiment approach 2
[0022] A manufacturing process of low-cost artificial travertine, comprising the following steps carried out in sequence: a. granulation, select one or more mixed commercially available slow-dissolving substances, slow-dissolving substances include A substance and C substance, preferably the Substance A: Substance C = 50:4. The substance A is a water-soluble powder, and the substance A is ammonium bicarbonate or urea. The substance C can be dissolved into a liquid only under acidic or alkaline conditions, and the substance C is an alkali-soluble acrylic resin at 45-55°C. Substance C contains water, and this part of water can dissolve 20-23% of substance A. The weight ratio of the total amount of slow-dissolving substances to the stone powder is 1:1.8-2.8 for uniform mixing, and the stone powder is 180-200 mesh stone powder. Granulate the mixture to produce frits or fused grains of different shapes and sizes; b. Block preparation, add the screened frits or fused grains to the...
Embodiment approach 3
[0024] A manufacturing process of low-cost artificial travertine, comprising the following steps carried out in sequence: a. granulation, select one or more mixed commercially available slow-dissolving substances, slow-dissolving substances include B substances and C substances, preferably B Substance: C substance = 50:3. The substance B is a water-soluble powder, and the substance B is polyacrylamide. The substance C can be dissolved into a liquid only under acidic or alkaline conditions, and the substance C is an alkali-soluble acrylic resin at 45-55°C. Substance C contains water, and this part of water can dissolve 27-45% of substance B. Mix evenly according to the weight ratio of the total amount of slow-dissolving substances to the stone powder at 1:3.2-4.5, and the stone powder is 200-315 mesh stone powder. Granulate the mixture to produce frits or fused grains of different shapes and sizes; b. Block preparation, add the screened frits or fused grains to the artificial...