Slow-seepage-resistant waterproof plugging mortar and preparation method thereof

A technology of waterproof plugging and sand leakage, which is applied in the field of waterproof building materials, can solve the problems of plastering mortar without heat resistance, fire prevention, bulging or cracks, waterproof failure, etc., achieve reasonable formula and production process design, improve mortar strength, Ease of use

Inactive Publication Date: 2021-11-09
河南省禹志建设工程有限公司
View PDF2 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] At present, plastering mortar generally does not have the performance of heat resistance and fire prevention. When a fire breaks out in a building, the temperature of the wall surface will change due to the fire. When the base concrete (or mortar) cracks, it will pull the paint to make it break, resulting in leakage of the building and failure of waterproofing. Buildings with brick-concrete or concrete structures, Due to structural deformation, hydration shrinkage of concrete (mortar), and thermal expansion and contraction, many cracks will occur.
This is a common problem in construction at present. Although scholars have made great efforts in various aspects, due to construction, maintenance and human factors, cracks in mortar and concrete are still inevitable.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] Take each component according to the following parts by weight: 30 parts of cement, 20 parts of sand, 5 parts of mineral admixture, 5 parts of superabsorbent polymer, 3 parts of water-soluble polymer, 1 part of water-based epoxy resin emulsion, water-based ring 1 part of oxygen curing agent, wherein the cement is a mixture of one or more of Portland cement or sulphoaluminate cement, and the mineral admixture is any one of fly ash, slag powder, silica fume or Various mixtures, the superabsorbent polymer is cross-linked sodium polyacrylate, and the water-soluble polymer adopts any one of polyacrylamide, polyvinyl alcohol, anionic polyacrylamide, and cationic polyacrylamide. The water-based epoxy resin emulsion is selected from one or more of EP-12S, EP-44, AERS6355, and YS8009. The specific preparation method is: first mix cement, sand, and mineral admixtures uniformly to obtain dry powder, and set aside; Put the superabsorbent polymer, water-soluble polymer, water-based ...

Embodiment 2

[0020] The components are taken according to the following parts by weight: 35 parts of cement, 25 parts of sand, 10 parts of mineral admixture, 6 parts of superabsorbent polymer, 4 parts of water-soluble polymer, 2 parts of water-based epoxy resin emulsion, water-based ring 2 parts of oxygen curing agent, wherein the cement is a mixture of one or more of Portland cement or sulphoaluminate cement, and the mineral admixture is any one of fly ash, slag powder, silica fume or Various mixtures, the superabsorbent polymer is cross-linked sodium polyacrylate, and the water-soluble polymer adopts any one of polyacrylamide, polyvinyl alcohol, anionic polyacrylamide, and cationic polyacrylamide. The water-based epoxy resin emulsion is selected from one or more of EP-12S, EP-44, AERS6355, and YS8009. The specific preparation method is: first mix cement, sand, and mineral admixtures uniformly to obtain dry powder, and set aside; Put the superabsorbent polymer, water-soluble polymer, wate...

Embodiment 3

[0022] Each component is taken according to the following parts by weight: 40 parts of cement, 30 parts of sand, 15 parts of mineral admixture, 7 parts of superabsorbent polymer, 5 parts of water-soluble polymer, 3 parts of water-based epoxy resin emulsion, water-based ring 3 parts of oxygen curing agent, wherein the cement is a mixture of one or more of Portland cement or sulphoaluminate cement, and the mineral admixture is any one of fly ash, slag powder, silica fume or Various mixtures, the superabsorbent polymer is cross-linked sodium polyacrylate, and the water-soluble polymer adopts any one of polyacrylamide, polyvinyl alcohol, anionic polyacrylamide, and cationic polyacrylamide. The water-based epoxy resin emulsion is selected from one or more of EP-12S, EP-44, AERS6355, and YS8009. The specific preparation method is: first mix cement, sand, and mineral admixtures uniformly to obtain dry powder, and set aside; Put the superabsorbent polymer, water-soluble polymer, water...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses slow-seepage-resistant waterproof leaking stoppage mortar and a preparation method thereof. The formula and the manufacturing process of the mortar are reasonable in design and convenient to use; cement, sand and mineral admixtures serve as composite gel components, and a water-borne epoxy resin emulsion and a water-borne epoxy curing agent can adjust the setting time of the mortar, so the strength, anti-permeability and other properties of the mortar are improved, and the mortar has good waterproof and anti-permeability properties; and in addition, a super absorbent polymer is wrapped by a water-soluble polymer to form a microcapsule, the super absorbent polymer does not participate in a reaction during stirring, mixing and cement solidification in virtue of the characteristic of slow dissolution of the water-soluble polymer, but the surface of the microcapsule is dissolved when mortar cracks and water flows into the microcapsule, so the water-absorbent polymer can quickly block cracks by utilizing the water absorption expansibility of the water-absorbent polymer, and a certain leakage self-repairing function is obtained.

Description

technical field [0001] The invention relates to the technical field of waterproof building materials, in particular to an anti-slow seepage waterproof plugging mortar and a preparation method thereof. Background technique [0002] With the advancement and development of grassroots construction and urbanization, the demand for plastering mortar used in building decoration projects is also increasing. Plastering mortar is a type of plastering mortar used to level or protect the base surface of the building Mortar, collectively referred to as mortar, is suitable for decoration of interior and exterior walls, cover surfaces, bottom surfaces, ceiling plastering, etc. of construction and decoration projects, and plays a protective and beautifying role. [0003] At present, plastering mortar generally does not have the performance of heat resistance and fire prevention. When a fire breaks out in a building, the temperature of the wall surface will change due to the fire. When the ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C04B28/06C04B111/27
CPCC04B28/06C04B2111/27C04B22/00C04B18/146C04B18/141C04B18/08C04B14/06C04B24/26C04B24/281
Inventor 梁军普杨新林梁栋梁随普杨康
Owner 河南省禹志建设工程有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products