Embodiment 1
[0045] A preparation method of a liquid floor color-changing decorative liquid, comprising the steps of:
[0046] 1) Add 1 part by weight of phthalocyanine green to the reaction kettle, then add 40 parts by weight of corn oil, 12 parts by weight of epoxy-modified silicone resin, heat up to 60°C, adjust the speed to 1200rpm, stir for 2 hours, and cool to room temperature , the density is 1.155g / ml, the viscosity is 8714CPS (25°C), and the green solution A is obtained;
[0047] 2) Add 2 parts by weight of anthocyanins to the reactor, add 40 parts by weight of deionized water, 8 parts by weight of short oil alkyd resin, and 10 parts by weight of ethanol, adjust the pH to 4.2, adjust the speed to 500rpm, and stir for 1 hour , the density is 1.023g / ml, the viscosity is 213CPS (25°C), and it is the red solution B;
[0048] 3) Add 1 part by weight of heat-sensitive orange dye to the reaction kettle, add 30 parts by weight of gasoline, adjust the rotation speed to 300rmp, and stir fo...
Embodiment 2
[0051] A preparation method of a liquid floor color-changing decorative liquid, comprising the steps of:
[0052] 1) Add 2 parts by weight of phthalocyanine green, 60 parts by weight of corn oil, and 15 parts by weight of epoxy-modified silicone resin into the reaction kettle, heat up to 80°C, adjust the speed to 1500rpm, stir for 3 hours, and cool to room temperature , the density is 1.165g / ml, the viscosity is 10134CPS (25°C), and the green solution A is obtained;
[0053] 2) Add 5 parts by weight of anthocyanins to the reactor, add 60 parts by weight of deionized water, 12 parts by weight of short oil alkyd resin, and 15 parts by weight of ethanol, adjust the pH to 4.4, adjust the speed to 800 rpm, and stir for 1.5 hours. The density was detected to be 1.037g / ml, and the viscosity was 431CPS (25°C), and the red solution B was obtained;
[0054] 3) Add 1.5 parts by weight of heat-sensitive orange dye to the reaction kettle, add 40 parts by weight of gasoline, adjust the rot...
Embodiment 3
[0057] A preparation method of a liquid floor color-changing decorative liquid, comprising the steps of:
[0058] 1) Add 3 parts by weight of phthalocyanine green, 80 parts by weight of corn oil, and 20 parts by weight of epoxy-modified silicone resin into the reaction kettle, heat up to 120°C, adjust the speed to 2000rpm, stir for 4 hours, and cool to room temperature , the density is 1.207g / ml, the viscosity is 12671CPS (25°C), and the green solution A is obtained;
[0059] 2) Add 8 parts by weight of anthocyanins to the reactor, add 80 parts by weight of deionized water, 15 parts by weight of short oil alkyd resin, and 20 parts by weight of ethanol, adjust the pH to 4.6, adjust the speed to 1200rpm, and stir for 2 hours , the density was 1.074g / ml, the viscosity was 728CPS (25°C), and the red solution B was obtained;
[0060] 3) Add 2 parts by weight of heat-sensitive orange dye to the reaction kettle, add 50 parts by weight of gasoline, adjust the rotation speed to 800rpm...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com