Anti-counterfeiting bill manufacturing method based on invisible image element recognition function
A technology of image elements and manufacturing methods, which is applied in the field of bills, can solve the problems that bills cannot be anti-counterfeited, and achieve the effect of preventing criminals from taking advantage of them
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] The manufacturing method of anti-counterfeiting bills based on the recognition function of invisible image elements includes the following steps:
[0023] Ingredients: 6 parts of sodium sulfate solution, 1 part of iodine solution, 10 parts of silver nitrate solution, 10 parts of ammonium sulfide solution, 3 parts of metal cation, 3 parts of non-metal anion, 3 parts of oxalic acid, 10 parts of potassium permanganate solution, ink 50 copies and 5 fluorescent pigments;
[0024] Mixing step: mixing 6 parts of sodium sulfate solution and 1 part of iodine solution through a mixing device to obtain a precipitation invisible ink, and then mixing 10 parts of silver nitrate solution and 10 parts of ammonium sulfide solution through a mixing device to obtain complex ion invisible ink, Then 3 parts of metal cations and 3 parts of non-metal anions are mixed by a mixing device to obtain a redox invisible ink, 3 parts of oxalic acid and 10 parts of potassium permanganate solution are ...
Embodiment 2
[0030] The manufacturing method of anti-counterfeiting bills based on the recognition function of invisible image elements includes the following steps:
[0031] Ingredients: 7 parts of sodium sulfate solution, 1.5 parts of iodine solution, 15 parts of silver nitrate solution, 15 parts of ammonium sulfide solution, 3.5 parts of metal cation, 3.5 parts of non-metal anion, 4 parts of oxalic acid, 15 parts of potassium permanganate solution, ink 75 copies and 6.5 copies of fluorescent pigments;
[0032] Mixing step: Mix 7 parts of sodium sulfate solution and 1.5 parts of iodine solution through a mixing device to obtain a precipitation type invisible ink, and then mix 15 parts of silver nitrate solution and 15 parts of ammonium sulfide solution through a mixing device to obtain complex ion type invisible ink, Then 3.5 parts of metal cations and 3.5 parts of non-metal anions are mixed by a mixing device to obtain a redox invisible ink, 4 parts of oxalic acid and 15 parts of potass...
Embodiment 3
[0038] The anti-counterfeiting bill manufacturing method based on the invisible image element recognition function includes the following steps:
[0039] Ingredients: 8 parts of sodium sulfate solution, 2 parts of iodine solution, 20 parts of silver nitrate solution, 20 parts of ammonium sulfide solution, 4 parts of metal cation, 4 parts of non-metal anion, 5 parts of oxalic acid, 20 parts of potassium permanganate solution, ink 100 copies and 8 fluorescent pigments;
[0040] Mixing step: mixing 8 parts of sodium sulfate solution and 2 parts of iodine solution through a mixing device to obtain a precipitation invisible ink, and then mixing 20 parts of silver nitrate solution and 20 parts of ammonium sulfide solution through a mixing device to obtain complex ion invisible ink, Then 4 parts of metal cations and 4 parts of non-metal anions are mixed by a mixing device to obtain a redox invisible ink, 5 parts of oxalic acid and 20 parts of potassium permanganate solution are mixed...