Environment protecting sprayed glue and its preparation and use
An environmentally friendly, glue-spraying technology, applied in the direction of adhesives, adhesive types, rosin adhesives, etc., can solve the problems of carcinogenicity, long drying time, high cost, etc., achieve large operating time flexibility, improve construction efficiency, and open time long effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0020] The present invention will be further described below with embodiment:
[0021] The optimum weight ratio of the spray glue is: thermoplastic elastomer SBS 8%, rosin 6%, hydrogenated rosin 7%, petroleum resin 4%, tackifying resin 3%, No. 6 extraction solvent oil 49.5%, acetone 5% , 15% cyclohexane, 2% butyl fat and 0.5% anti-aging agent.
[0022] The processing method of making environment-friendly glue spray of the present invention is as follows:
[0023] a. First put quantitative No. 6 extraction solvent oil, acetone, and cyclohexane into the agitator, and start the machine to stir evenly to form a mixed solution;
[0024] b. Put a certain amount of thermoplastic elastomer SBS into the stirrer and stir;
[0025] c. Finally, put quantitative rosin, hydrogenated rosin, petroleum resin, tackifying resin, butyl fat and anti-aging agent into the stirrer and stir;
[0026] d. Put all the above materials into the mixer and continue to stir and dissolve at room temperature...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com