Nanometer polypropylene modifier and its prepn process
A polypropylene and modifier technology, applied in the field of nano-polypropylene modifier, can solve the problems of increased production cost, single function, large material loss, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] 1. Put each component of the present invention into a cantilever double-helix cone mixer according to the following weight ratio for premixing and extensive dispersion:
[0037] Nano fully vulcanized powder rubber: 40%, antioxidant 168: 15%, antioxidant 1010: 15%, dispersant: 5%, antistatic agent 477: 5%, coupling agent: 10%, calcium stearate 10%.
[0038] The operating speed of the cantilever double-helix cone mixer is: 100-150 revolutions per minute, and the mixing time is 40 minutes.
[0039] 2. After premixing and coarse dispersion, put the raw materials into the horizontal ball mill to refine and disperse the raw materials. The process control speed of the horizontal ball mill is 45-50 revolutions per minute.
[0040] 3. After refining and dispersing, put the raw materials into the twin-screw granulator to extrude and granulate to further strengthen the dispersing. During granulation, the material temperature in the twin-screw granulator is controlled within the...
Embodiment 2
[0042] The component of embodiment 2 and the step of preparation process are identical with embodiment 1, and difference is:
[0043] The weight ratio of each component is: Nano fully vulcanized powder rubber: 45%, antioxidant 168: 10%, antioxidant 1010: 15%, dispersant: 5%, antistatic agent 477: 5%, coupling agent : 10%, calcium stearate 10%.
[0044] Due to the addition of 5% nanometer fully vulcanized powdered rubber, the stirring time of step 1) was increased to 60 minutes.
Embodiment 3
[0046] The component of embodiment 3 and the step of preparation process are identical with embodiment 1, difference is:
[0047] The weight ratio of each component is: Nano fully vulcanized powder rubber: 50%, antioxidant 168: 10%, antioxidant 1010: 10%, dispersant: 5%, antistatic agent 477: 5%, coupling agent : 10%, calcium stearate 10%.
[0048] Due to the addition of 5% nanometer fully vulcanized powdered rubber, the stirring time of step 1) was increased to 80 minutes.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com