A production method and a seedling-strengthening agent technology, which are applied in the field of agricultural rice seedling raising, can solve the problems of low nutrient utilization rate, insufficient effect of promoting seed germination and seedling emergence, etc., and achieve the effect of improving the comprehensive quality of seedlings
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] 1. Select oblique gray-green zeolite powder (passing 80 mesh) and adopt rolling oxygen calcination, the temperature is 80-300 ℃, the time is 1.5-2 hours, and the addition amount is 46.63%
[0014] 2. Industrial sulfuric acid 26%
[0015] 3. Take 11% ammonium sulfate, 9% diammonium phosphate, 5% potassium sulfate, and 1% zinc sulfate respectively, mix them thoroughly and stir well
[0016] 4. Take trace elements: 100 grams of ferrous sulfate, 14 grams of boric acid, 10 grams of manganese sulfate, 1 gram of copper sulfate, 0.5 grams of ammonium molybdate, mix the five compounds thoroughly, stir well, take 0.2%
[0017] 5. Take 0.9% of Dixon and 0.27% of Jiashuangling respectively, mix them well and stir evenly
[0018] 6. Add step 2 to step 1, mix well and stir evenly. Stuffy for 2-3 days
[0019] 7. Add step 4 to step 3, mix well and stir evenly
[0020] 8. Add step 7 to step 6, mix well and stir evenly
[0021] 9. Finally, step 5 is added to step 8, and the present...
Embodiment 2
[0024] 1. Select clinoptilolite gray-green zeolite (0.25-0.5mm particle size) by rolling oxygen calcination, the temperature is 80-300°C, the time is 1.5-2 hours, and the addition amount is 56.33%.
[0025] 2. Industrial sulfuric acid 10%, after immersion, immerse for 2-3 days, drain out and dry.
[0026] 3. Take ammonium sulfate 27%, diammonium phosphate 9%, potassium sulfate 5%, and zinc sulfate 1% respectively
[0027] 4. Take trace elements: 100 grams of ferrous sulfate, 14 grams of boric acid, 10 grams of manganese sulfate, 1 gram of copper sulfate, 0.5 grams of ammonium molybdate, mix the five compounds thoroughly, stir evenly, and weigh 0.5%
[0028] 5. Take 0.9% of Dixon and 0.27% of Jiashuangling respectively, mix them well and stir evenly
[0029] 6. Add process 2 to process 1, fully mix and stir evenly, and suffocate for 2-3 days
[0030] 7. Add step 4 to step 3, mix well and stir evenly
[0031] 8. Add step 7 to step 6, mix well and stir evenly
[0032] 9. Fina...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com