[0027] (1) First, dissolve 1 part of PVP-K3O in an equal amount of deionized water, heat and stir at 60°C for 0.5 hours to obtain a PVP-K30 solution; (2) Prepare from 1 part of triethanolamine and 1 part of deionized water pH adjuster; (3) dilute 2 parts of thickener HISOLD 206 with 16 parts of deionized water, add 2 parts of triethanolamine, stir to make it swell to completely transparent, and obtain neutralized HI SOLD 206; (4) take 10 parts 200 parts of polyethylene glycol and 10 parts of propylene glycol are mixed to make water-soluble low-carbon alcohol; (5) according to 0.5 parts of dispersant AEC 9 -H, 0.15 parts of wetting agent PE-100, PVP-K30 solution prepared in the first step, 0.5 parts of oleic acid, water-soluble low-carbon alcohol prepared in the fourth step, 0.05 parts of 1,2,3-benzene Triazole and 20 parts of deionized water are prepared into a mixed solution, which is stirred evenly to form a slurry, and then 8 parts of phthalocyanine blue are added and knead...
Embodiment 2
[0029] (1) First, 2 parts of PVP-K30 and 1 part of PVP-K15 were dissolved in an equal amount of deionized water, heated and stirred at 80°C for 1 hour to obtain a PVP-K30 solution and a PVP-K15 solution; (2) by 1 part of triethanolamine and 1 part of deionized water are prepared as a pH regulator; (3) Dilute 0.5 part of thickener HI SOLD 206 with 4 parts of deionized water, add 0.5 part of triethanolamine, and then add 0.5 part of thickener HISOLD 105 was diluted with 9 parts of deionized water, then added 0.5 parts of triethanolamine, stirred to make it completely transparent, and neutralized HISOLD 206 and neutralized HISOLD 105 were obtained; (4) Take 15 parts of polyethylene glycol and 15 parts of propylene glycol Mix to make water-soluble low-carbon alcohol; (5) According to 1 part of dispersant AEC 9 -H, 0.5 parts of wetting agent PE-100, PVP-K30 solution prepared in the first step, PVP-K15 solution, 2 parts of oleic acid, water-soluble low-carbon alcohol prepared in the...
Embodiment 3
[0031] (1) First, dissolve 6 parts of PVP-K30 in the same amount of deionized water, heat and stir at 70°C for 0.5 hours to obtain a PVP-K30 solution; (2) Prepare from 1 part of triethanolamine and 1 part of deionized water pH adjuster; (3) Dilute 0.5 parts of thickener HISOLD 206 with 4 parts of deionized water, add 0.5 parts of triethanolamine, stir to make it swell to completely transparent, and obtain neutralized HI SOLD 206; (4) Take 10 Parts of polyethylene glycol 200, 5 parts of polyethylene glycol 400, 10 parts of glycerin are formulated into water-soluble low-carbon alcohols; (5) according to 0.8 parts of dispersant AEC 9-H, 0.3 parts of wetting agent PE-100, PVP-K30 solution prepared in the first step, 1 part of oleic acid, water-soluble low-carbon alcohol prepared in the fourth step, and 1 part of 1,2,3-benzene Triazole and 15 parts of deionized water are prepared into a mixed solution, which is stirred evenly to form a slurry, and then 10 parts of phthalocyanine bl...