Cardboard starch gum activating agent and cardboard starch gum
A technology of active agent and starch glue, applied in the field of cardboard starch glue active agent and cardboard starch glue, can solve the problems of increased working hours, pollution, difficult product stability, separation and precipitation of water glue, etc., and achieves simple manufacturing process, stable product quality, The effect of strong adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The activator of the present embodiment is formed by uniformly mixing the following weight percentages:
[0016] 70% of sepiolite powder, wherein the content of sepiolite is 85%, and the particle size is 800 mesh;
[0017] Light calcium powder 20%, particle size is 1200 mesh;
[0018] Mortar plasticizer 2.5%, "Guchuang" brand WF type mortar agent produced by Lishuyuan New Building Material Factory;
[0019] Sodium carboxymethyl cellulose 5%, industrial grade;
[0020] White granulated sugar 2.5%, civil grade;
[0021] The active agent of this embodiment is obtained after uniformly mixing the above ingredients. Then add it to commercially available ordinary cardboard starch glue and stir evenly, the amount of active agent added is 1% of the weight of starch glue
Embodiment 2
[0023] The activator of the present embodiment is formed by uniformly mixing the following weight percentages:
[0024] 75% of sepiolite powder, wherein the content of sepiolite is 70%, and the particle size is 1200 mesh;
[0025] Light calcium powder 10%, particle size is 1000 mesh;
[0026] Mortar plasticizer 5%, is the mortar plasticizer containing naphthalenesulfonic acid sodium formaldehyde condensate;
[0027] Sodium carboxymethyl cellulose 6%, industrial grade;
[0028] White granulated sugar 1%, civil grade;
[0029] Fly ash 3%;
[0030] The active agent of this embodiment is obtained after uniformly mixing the above ingredients. Then add it to commercially available ordinary cardboard starch glue and stir evenly, the amount of active agent added is 3% of the weight of starch glue
Embodiment 3
[0032] The activator of the present embodiment is formed by uniformly mixing the following weight percentages:
[0033] Sepiolite powder 65%, wherein the content of sepiolite is 78%, and the particle size is 1000 mesh;
[0034] Light calcium powder 15%, particle size is 800 mesh;
[0035] 1% mortar plasticizer, mortar plasticizer containing sodium dodecyl sulfonate;
[0036] Sodium carboxymethyl cellulose 3%, industrial grade;
[0037] White granulated sugar 5%, civil grade;
[0038] Bentonite 11%;
[0039] The active agent of this embodiment is obtained after uniformly mixing the above ingredients. Then add it to commercially available ordinary cardboard starch glue and stir evenly, the amount of active agent added is 6% of the weight of starch glue
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology