[0017] Preparation of the transparent covering layer (1): Place 15-20 parts of the prepared 8% polyvinyl alcohol aqueous solution in a dispersion tank, add 35-40 parts of ethylene-propylene emulsion under stirring conditions, and then add 2 10-15 parts of % hydroxyethyl cellulose aqueous solution and 10 parts of light-curable acrylic thickener, and the aqueous solution containing 0.08-0.1% sodium pentachlorophenate was added to 100 parts under stirring conditions.
[0018] Preparation of transparent covering layer (2): Put 15-20 parts of the prepared 5% polyvinyl formal aqueous solution in the dispersion tank, add 35-40 parts of styrene-acrylic emulsion under stirring conditions, and then Add 10-15 parts of 2% hydroxyethyl cellulose aqueous solution and 10 parts of light-curable acrylic thickener, and make up the parts to 100 parts with the aqueous solution containing 0.08-0.1% sodium pentachlorophenate under stirring condition.
[0019]Preparation of transparent covering laye...
Embodiment 2
[0021] Preparation of colored covering layer (1): Place 15 to 20 parts of the prepared 8% polyvinyl alcohol aqueous solution in a dispersion tank, then add 20 parts of aqueous solution containing 0.08 to 0.1% sodium pentachlorophenate and 10% sodium hexametaphosphate 1 part, slowly add 1 part of activated clay, 5 parts of titanium dioxide, 4 parts of light calcium carbonate and 4 parts of talc under stirring conditions. After completion, add a little aqueous solution containing 0.1% tributyl phosphate for defoaming treatment, and then Add 5 parts of titanium dioxide and 4 parts of light calcium carbonate under certain conditions, and then add a little aqueous solution containing 0.1% tributyl phosphate for defoaming treatment. Add 25~30 parts of ethylene-propylene emulsion under the condition of stirring, and then add 10~15 parts of 2% hydroxyethyl cellulose aqueous solution and 10 parts of light-curable acrylic thickener, and make up the parts with water after stirring evenly ...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com