Technology of dying granite stone blue or green
A granite and stone technology, applied in the direction of pigment slurry, etc., can solve the problems of poor heat and weather resistance of blue varieties, easy to lose color, unable to obtain blue varieties, etc., and achieve the effect of simple and practical equipment and low cost.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Off-white fine flower 603 produced in Fujian # Granite (10×10×2CM 3 ) surface of the sample was cleaned, dried in an oven at 120°C for 2 hours, and then placed in liquid A (potassium ferrocyanide 42 g / L, sodium lauryl sulfate 1 g / L, water remaining amount) dipping tank for 5 hours, take it out, drain the remaining liquid on the surface, put it in an oven and bake it at 120°C for 2 hours, and then dip into liquid B (ferric chloride 50 g / L, lauryl sulfuric acid Sodium 1 g / L, water balance) for 5 hours, take it out, drain the remaining liquid on the surface, bake in the oven at 120°C for 2 hours, polish the stone surface slightly after taking it out, dry it, and apply 201 methyl Silicone oil can get blue granite stone.
Embodiment 2
[0030] The "Leopard Skin Flower" granite (30×30×2CM) produced in Sichuan 3 ) surface of the sample was cleaned, dried in an oven at 120°C for 2 hours, then placed in an immersion tank filled with liquid A (the formula is the same as in Example 1) and soaked for 5 hours, after taking it out, drain the remaining liquid on the surface, and place Bake in an oven at 120°C for 2 hours, then dip into solution B (ferric nitrate 45 g / L, sodium lauryl sulfate 1 g / L, water balance) for 5 hours, take it out and drain the remaining surface. Liquid, bake in an oven at 120°C for 2 hours, take it out, polish the surface of the stone, dry it, and apply 201 methyl silicone oil to get green granite stone.
Embodiment 3
[0032] Gray and white fine flower 603# granite (10×10×2CM) produced in Fujian 3 ) sample to clean the surface, dry it in an oven at 120°C for 2 hours, then place it in a pressurizable airtight impregnation tank to pressurize (pressure 1Mpa, constant pressure 1-1.5 hours) and impregnate A liquid (A liquid formula Same as Example 1), take it out and put it in an oven, bake it at 120°C for 2 hours, then put it in another closed dipping tank and pressurize it (pressure 1Mpa, constant pressure 1-1.5 hours) to impregnate B liquid (B liquid The formula is the same as in Example 1), after taking it out, drain the remaining liquid on the surface, bake it in an oven at 120°C for 2 hours, after taking it out, polish the stone surface slightly, dry it, and apply 201 methyl silicone oil to get the blue flower Granite stone.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com