Warp-knitted base sun shading material and preparation method thereof
A technology of warp knitting and knitting base cloth, which is applied in the field of building decoration materials, can solve problems such as single means and weak creativity, and achieve the effects of good optical performance, effective heat insulation and good visibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Embodiment 1, the preparation of white warp-knitted base silver sunshade material
[0017] (1) Provide polyester warp knitted base fabric;
[0018] (2) Carry out white PVC slurry coating on described polyester warp-knitted base cloth, dry, obtain intermediate material;
[0019] Wherein, the white PVC slurry includes the following components by weight: polyvinyl chloride: 100 parts, DINP: 51 parts, Ba-Zn liquid stabilizer: 3 parts, pigment slurry: 30 parts, flame retardant ethane- 1, 2 bis(pentabromobenzene): 14 parts, antimony trioxide: 36 parts, antimold additive ABF-5-DIDP: 1 part.
[0020] When configuring, add DINP and Ba-Zn liquid stabilizer into the barrel, then add polyvinyl chloride, flame retardant and anti-mold additives in turn under stirring, and stir for 10 minutes to complete the premixing; then grind with three rollers Machine for grinding, filtered and stored in another clean bucket. Then according to the color required by the product, add the color p...
Embodiment 2
[0025] Embodiment two, the preparation of blue warp knitted base silver sunshade material
[0026] (1) Provide polyester warp knitted base fabric;
[0027] (2) Carry out blue PVC slurry coating on described polyester warp-knitted base cloth, dry, obtain intermediate material;
[0028] Wherein, the blue PVC slurry includes the following components by weight: polyvinyl chloride: 100 parts, DINP: 55 parts, calcium-zinc liquid stabilizer: 2.5 parts, pigment slurry: 20 parts, flame retardant ethane -1,2 bis(pentabromobenzene): 14 parts, antimony trioxide: 36 parts, antimold additive ABF-5-DIDP: 1.5 parts.
[0029] When configuring, add DINP and calcium-zinc liquid stabilizer into the barrel, then add polyvinyl chloride, flame retardant and anti-mold additives in turn under stirring, and stir for 10 minutes to complete the premixing; then grind with three rollers Machine for grinding, filtered and stored in another clean bucket. Then according to the color required by the product...
Embodiment 3
[0034] Embodiment three, the preparation of green warp knitted base silver sunshade material
[0035] (1) Provide polyester warp knitted base fabric;
[0036] (2) Carry out blue PVC slurry coating on described polyester warp-knitted base cloth, dry, obtain intermediate material;
[0037]Wherein, the green PVC slurry includes the following components by weight: polyvinyl chloride: 100 parts, plasticizer DOP: 53 parts, calcium-zinc liquid stabilizer: 2.5 parts, pigment slurry: 24 parts, ethane- 1, 2 bis(pentabromobenzene): 14 parts, antimony trioxide: 36 parts, antimold additive ABF-5-DIDP: 1 part.
[0038] When configuring, add DINP and calcium-zinc liquid stabilizer into the barrel, then add polyvinyl chloride, flame retardant and anti-mold additives in turn under stirring, and stir for 10 minutes to complete the premixing; then grind with three rollers Machine for grinding, filtered and stored in another clean bucket. Then according to the color required by the product, ad...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction