Process for preparing potash magnesium sulphate fertilizer by muddy potassium mixed salt mineral
A technology of potassium magnesium sulfate fertilizer and potassium mixed salt ore, which is applied in the production process field of potassium magnesium sulfate fertilizer, can solve the problems of not meeting quality requirements, poor quality of potassium magnesium fertilizer, low recovery rate of potassium magnesium fertilizer, etc., and achieves Ease of operation, high recovery rate, and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Embodiment 1, a kind of technique that utilizes primary potassium mixed salt ore to produce potassium magnesium sulfate fertilizer, its steps are as follows:
[0026] (1) After the original potassium mixed salt ore is mined, it is crushed to less than 4 mm. Under normal temperature conditions, the ore is first added to a scrubbing bucket with stirring to wash the ore. The ore washing medium is saturated brine, and the mass concentration of the ore is 20%. Washing time is 5 minutes;
[0027] (2) Sieve the washed pulp with a 60-mesh vibrating sieve, the under-sieve will settle naturally, and the brine after clarification will be returned to the next ore washing; the over-sieve will be ground, and the grinding mass concentration will be 50%;
[0028] (3) Add the fine mud inhibitor to the potassium mixed salt after ore grinding, and then add the collector to enrich the potassium-containing mineral langbeinite by flotation, and the obtained concentrate is coarse potassium an...
Embodiment 2
[0030] Embodiment 2, a kind of technique that utilizes primary potassium mixed salt ore to produce potassium magnesium sulfate fertilizer, its steps are as follows:
[0031] (1) After the original potassium mixed salt ore is mined, it is crushed to less than 4 mm. Under normal temperature conditions, the ore is first added to a scrubbing bucket with stirring to wash the ore. The ore washing medium is saturated brine, and the mass concentration of the ore is 60%. Washing time is 60 minutes;
[0032] (2) Sieve the washed pulp with a 200-mesh vibrating sieve, the under-sieve will settle naturally, and the brine after clarification will be returned to the next ore washing; the over-sieve will be ground, and the grinding mass concentration will be 60%;
[0033] (3) Add the fine mud inhibitor to the potassium mixed salt after ore grinding, and then add the collector to enrich the potassium-containing mineral langbeinite by flotation, and the obtained concentrate is coarse potassium ...
Embodiment 3
[0035] Embodiment 3, a kind of technique that utilizes primary potassium mixed salt ore to produce potassium magnesium sulfate fertilizer, its steps are as follows:
[0036] (1) After the original potassium mixed salt ore is mined, it is crushed to less than 4mm. Under normal temperature conditions, the ore is first added to a scrubbing bucket with stirring to wash the ore. The ore washing medium is saturated brine, and the ore washing mass concentration is 40%. Washing time is 30 minutes;
[0037] (2) Screen the washed ore pulp with a 150-mesh vibrating sieve, and the under-sieve will settle naturally, and the brine after clarification will be returned to the next ore washing; the over-sieve will be ground, and the grinding mass concentration will be 55%;
[0038] (3) Add the fine mud inhibitor to the potassium mixed salt after ore grinding, and then add the collector to enrich the potassium-containing mineral langbeinite by flotation, and the obtained concentrate is coarse p...
PUM