A brine and mud technology, which is applied in the field of saturated brine slurry and its preparation, can solve the problems of high mud cost, reducing the use of solid powder weighting materials, and difficult maintenance, etc., to solve the problem of irregular well diameter, inhibit corrosion, and reduce well diameter Extended effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0058] Get 100mL brine solution, the specific gravity of the brine solution is 1.28, add NaCl to the brine solution under stirring conditions until saturated, then add 2g anti-saline soil, 8g sulfomethyl phenolic resin, 1g Sulfomethyl lignite, 1.0g hydroxyethyl cellulose, stir for 10-15 minutes to mix. The specific gravity of the obtained brine slurry was 1.42, the plastic viscosity was 6 mPas, the dynamic shear force was 4 Pa, and the API fluid loss was 8 mL.
[0059] It shows that the fluid loss and rheological properties of the salt water slurry described in the present invention are good.
Embodiment 2
[0061] Get 100mL brine solution, the specific gravity of the brine solution is 1.25, add NaCl to the brine solution under stirring conditions until saturated, then add 9g attapulgite and 2g sulfomethyl phenolic resin to the saturated brine solution, 5g sulfomethyl lignite, 0.2g hydroxyethyl cellulose, stir for 10-15 minutes to mix. The obtained brine slurry had a specific gravity of 1.43, a plastic viscosity of 8 mPas, a dynamic shear force of 6 Pa, and an API fluid loss of 9 mL.
[0062] It shows that the fluid loss and rheological properties of the salt water slurry described in the present invention are good.
Embodiment 3
[0064] Get 100mL brine solution, the specific gravity of the brine solution is 1.25, add NaCl to the brine solution under stirring conditions until saturated, then add 4g sepiolite, 6g sulfomethyl phenolic resin, 2g Sulfomethyl lignite, 0.8g hydroxyethyl cellulose, stir for 15-20 minutes to mix. The obtained brine slurry had a specific gravity of 1.43, a plastic viscosity of 7 mPas, a dynamic shear force of 6 Pa, and an API fluid loss of 8 mL.
[0065] It shows that the fluid loss and rheological properties of the salt water slurry described in the present invention are good.