A cooling fluid and water lubrication technology, applied in lubricating compositions, petroleum industry, etc., can solve the problems of limited application of water-based metalworking fluids, poor lubricity and corrosion resistance, unstable chemical properties, etc., to improve occupational health. , Good chemical corrosion resistance and obvious lubricating effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032]The water-lubricated wear-resistant coolant consists of the following percentage components in parts by weight:
[0033] Water 89.5g
[0034] HM-55 Closed System High Temperature Antirust Liquid 8.5g
[0035] Carbon nanotubes 0.2g
[0036] Graphite 1.8g
[0037] The preparation method of water-lubricated wear-resistant coolant: use 89.5g of water as the main raw material, add 0.2g of carbon nanotubes, 8.5g of HM-55 closed system high-temperature resistant anti-rust liquid, and 1.8g of graphite, and stir at high speed with the equipped stirring equipment Ready in 30 minutes.
Embodiment 2
[0039] The water-lubricated wear-resistant coolant consists of the following percentage components in parts by weight:
[0040] Water 87.5g
[0041] VpCI-377 high temperature antirust liquid 10g
[0042] n-Cu 0.5g
[0043] Graphite 2g
[0044] The preparation method of water-lubricated wear-resistant coolant: use 87.5g of water as the main raw material, add n-Cu 0.5g, VpCI-377 high temperature resistant anti-rust liquid 10g, graphite 2g, and stir at high speed for 30 minutes with the equipped stirring equipment Prepared.
Embodiment 3
[0046] The water-lubricated wear-resistant coolant consists of the following percentage components in parts by weight:
[0047] Water 81.9g
[0048] 787B Closed System Cooling Water Antirust Liquid 15g
[0049] n-Ph 1g
[0050] Graphite 2.1g
[0051] The preparation method of water-lubricated wear-resistant coolant: use 81.9g water as the main raw material, add n-Ph 1g, 787B closed system cooling water anti-rust liquid 15, graphite 2.1g, and stir for 30 minutes at high speed with the equipped stirring equipment Prepared.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com