Welding process of three-way valve seat and valve body
A technology of welding process and three-way valve, which is applied in welding equipment, manufacturing tools, arc welding equipment, etc., can solve the problems of difficult welding and achieve the effects of avoiding post-weld cracking, ensuring weld quality, and improving organization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0017] A three-way valve seat and valve body welding process, the process is:
[0018] 1. Use ER90S-G welding wire;
[0019] 2. Clean up the dirt near the groove and the groove;
[0020] 3. Preheating: the temperature is 150-200°C;
[0021] 4. Multi-layer welding is adopted, and the multi-layer rear layer dehydrogenates the front layer. The temperature between the control layers cannot be lower than the preheating temperature, and the temperature between the layers is controlled at 200-250 °C;
[0022] 5. Control heat input: use small welding current and faster welding to control heat input. The welding current is 220-240A, the welding voltage is 13-15V, and the welding speed is 100-150mm / min;
[0023] 6. Inert gas protection: the gas flow rate is 10-15L / min;
[0024] 7. Post-heat treatment: post-heat treatment is carried out immediately after welding, the post-heating temperature is 300°C, and the heat preservation time is 1h.
[0025] 8. Heat trea...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com