Low production cost environmental protection type snow removing agent
A production cost and environmentally friendly technology, applied in other chemical processes, chemical instruments and methods, etc., can solve the problems of polluted groundwater, non-environmental protection, construction, road corrosion damage, etc., to reduce maintenance costs, prevent freezing, The effect of low production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] An environment-friendly deicing agent with low production cost, which is composed of the following components in the following parts by weight: 50 kg of calcium chloride, 20 kg of sodium tetraborate, 20 kg of urea, 15 kg of sodium nitrite, peroxide 8 kg of sodium sulfate. The preparation method of the deicing agent is as follows: mixing the above-mentioned raw materials according to the above-mentioned weight, and then adding the mixture into water at 70° C. to make a saturated solution.
Embodiment 2
[0012] An environment-friendly deicing agent with low production cost is composed of the following components according to the following ratios in parts by weight: 70 kg of calcium chloride, 12 kg of sodium tetraborate, 15 kg of urea, 8 kg of sodium nitrite, peroxide Sodium sulfate 5 kg. The preparation method of the deicing agent is as follows: mixing the above-mentioned raw materials according to the above-mentioned weight, and then adding the mixture into water at 70° C. to make a saturated solution.
Embodiment 3
[0014] An environment-friendly deicing agent with low production cost is composed of the following components according to the following ratios in parts by weight: 90 kg of calcium chloride, 5 kg of sodium tetraborate, 10 kg of urea, 5 kg of sodium nitrite, peroxide Sodium sulfate 3 kg. The preparation method of the deicing agent is as follows: mixing the above-mentioned raw materials according to the above-mentioned weight, and then adding the mixture into water at 70° C. to make a saturated solution.