Embodiment 1
[0013] Leveling agent for wool and silk, including the following raw materials in parts by mass: 8 parts of fatty amine polyoxyethylene ether, 5 parts of sodium benzylnaphthalene sulfonate, 2 parts of polyvinylpyrrolidone, 4 parts of stearic acid, and 6 parts of urea , 15 parts of water, 30 parts of ethylene glycol.
[0014] The preparation method of this example is as follows: according to the mass ratio, add urea and water into the reactor in sequence, stir for 10 minutes, then add ethylene glycol, fatty acid, fatty amine polyoxyethylene ether, sodium benzyl naphthalene sulfonate and polyvinylpyrrolidone in sequence Stir at a speed of 800 rpm for 20 minutes to obtain a leveling agent for wool and silk.
Embodiment 2
[0016] Leveling agent for wool and silk, including the following raw materials in parts by mass: 10 parts of fatty amine polyoxyethylene ether, 8 parts of sodium benzylnaphthalene sulfonate, 4 parts of polyvinylpyrrolidone, 7 parts of stearic acid, and 8 parts of urea , 18 parts of water, 35 parts of ethylene glycol.
[0017] The preparation method of this example is as follows: according to the mass ratio, add urea and water into the reactor in sequence, stir for 10 minutes, then add ethylene glycol, fatty acid, fatty amine polyoxyethylene ether, sodium benzyl naphthalene sulfonate and polyvinylpyrrolidone in sequence Stir at a speed of 1000 rpm for 30 minutes to obtain a leveling agent for wool and silk.
Embodiment 3
[0019] Leveling agent for wool and silk, including the following raw materials in parts by mass: 9 parts of fatty amine polyoxyethylene ether, 7 parts of sodium benzylnaphthalene sulfonate, 3 parts of polyvinylpyrrolidone, 6 parts of stearic acid, and 7 parts of urea , 16 parts of water, 32 parts of ethylene glycol.
[0020] The preparation method of this example is as follows: according to the mass ratio, add urea and water into the reactor in sequence, stir for 10 minutes, then add ethylene glycol, fatty acid, fatty amine polyoxyethylene ether, sodium benzyl naphthalene sulfonate and polyvinylpyrrolidone in sequence Stir at a speed of 1000 rpm for 30 minutes to obtain a leveling agent for wool and silk.
[0021] The leveling agent of the present invention is suitable for coloring and leveling dyeing of wool and real silk, and the wool and real silk treated with the leveling agent of the present invention have uniform dyeing and good leveling property, and the dye uptake rate...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com