Compressed glulam and production method of compressed glulam
A production method and technology for glulam, applied in wood compression, wood processing appliances, manufacturing tools, etc., can solve problems such as high cost and complex equipment, and achieve the effect of increasing density, increasing strength, and eliminating the need for processing and cutting
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment 1
[0042] To produce a square compressed glulam with a length of 2 meters and a section of 15 centimeters, the following method steps can be used:
[0043] Step 1. Install an open die with a corresponding section, and taper is provided in the open die.
[0044] Step 2, billet assembly: Determine the average density of the product to be 0.7 g / cubic centimeter, weigh the corresponding amount, skinless, relatively straight, small-diameter wood with a diameter of about 4 cm, a length of 2 meters, and a moisture content of 20%. It is best to use tree species with similar densities, with a lot of resin, and those with poor bonding performance cannot be used. The raw materials are preferably plantation fast-growing woods, such as eucalyptus, poplar and fir, etc.), and the big and small heads are placed alternately and bundled well.
[0045] Step 3, softening with steam above 100°C for 30-60 minutes;
[0046] Step 4. Dip in a relatively low-viscosity phenolic resin with a solid content ...
specific Embodiment 2
[0053] To produce a compressed glulam bamboo square with a length of 2 meters and a section size of 15 cm x 13 cm, the following steps are included:
[0054] 1. Install the corresponding section mold;
[0055] 2. Preparation: Cut the 2-meter-long moso bamboo section into 4 pieces, remove the inner and outer sections, flatten, and remove the green bamboo yellow (the thickness does not need to be determined, the thickness can be different within the same piece or between bamboo pieces), and air-dried to a moisture content of 25 %about;
[0056] 3. Blank assembly: the density after compression and integration is 0.8g / cm 3 , Weigh the corresponding amount of bamboo slices: place layers evenly, alternate sizes, and the section size after binding is 2-3cm larger than the size after compression.
[0057] The subsequent steps are the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com