Yellow-light environment-friendly cooling coating
A heat-dissipating coating, green technology, applied in the direction of powder coating, coating, etc., can solve the problems of weak surface adhesion, small application range, unsatisfactory use effect, etc., and achieve low cost, good construction and strong heat dissipation performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A kind of yellow light green heat-dissipating coating is characterized in that it is made up of the raw material of following parts by weight (kg):
[0017] SG-4 type PVC resin 92, fast extrusion carbon black 4, 1-hydroxycyclohexyl phenyl ketone 0.5, N,N-diethylaniline 0.3, polybenzimidazole 1, glass fiber 2-triethylene glycol 2 , Hydroxyethylidene diphosphonic acid 2, lanthanum oxide 0.3, sepiolite powder 13, polyvinyl acid 1, phthalocyanine green 3, modification additive 4;
[0018] The modified filler is composed of the following raw materials in parts by weight:
[0019] Pyrophyllite 20, diatomite 40, alum powder 3, jade powder 6, disodium octaborate tetrahydrate 3, didecyldimethylammonium bromide 0.8, calcium acetylacetonate 2, diacetone alcohol 2;
[0020] Calcinate the above diatomite at 500°C for 1 hour, cool to room temperature, add disodium octaborate tetrahydrate and pyrophyllite, mix and grind for 30 minutes, add diacetone alcohol and calcium acetylacetonat...