Embodiment 1
[0021] Production of zinc hydroxide: After dissolving and leaching zinc from zinc-based alloy copper plating waste with excess sulfuric acid solution, the resulting zinc-containing solution is filtered and the filtrate obtained is purified to remove impurities, and the acidic purification solution obtained is the acidic zinc-containing solution for use: In addition, take the zinc-based alloy electroplating copper waste and add excess sodium hydroxide to stir to dissolve, and then filter the obtained zinc-containing liquid and then purify and remove impurities to obtain an alkaline zinc-containing liquid purification liquid, which is alkaline zinc-containing liquid, for subsequent use; The zinc-containing liquid and the above-mentioned alkaline zinc-containing liquid are mixed and reacted in a ratio of 1:1, and the obtained liquid is filtered after the reaction, and the obtained filter cake is washed with water for 2 to 3 times, and then dried at 130°C for 1.2h, and the obtained ...
Embodiment 2
[0023] Production of zinc oxide: After dissolving nickel-melted zinc slag with excess sulfuric acid solution to leach zinc, the obtained zinc-containing solution is filtered and the filtrate is purified to remove impurities, and the acidic purification solution is the acidic zinc-containing solution. Add excess sodium hydroxide to the zinc slag and stir to dissolve, filter the obtained zinc-containing liquid and then purify and remove impurities to obtain an alkaline zinc-containing liquid purification liquid, which is alkaline zinc-containing liquid, for subsequent use; The neutral zinc-containing solution is mixed according to the ratio of 1:1 for reaction. After the reaction, the obtained liquid is filtered, and the obtained filter cake is washed with water for 2 to 3 times, and then dried at 120°C for 1 hour. The obtained is zinc hydroxide, and then the hydrogen Zinc oxide is dried at 120°C for 1 hour to obtain the product. The obtained zinc oxide can be active zinc oxide o...
Embodiment 3
[0025] Production of elemental zinc: After dissolving and leaching zinc from the molten sponge copper waste with excess sulfuric acid solution, the resulting zinc-containing solution is filtered and the filtrate is purified to remove impurities, and the acidic purification solution is the acidic zinc-containing solution. Add excess sodium hydroxide to the sponge copper and molten zinc fume and stir to dissolve, then filter the obtained zinc-containing liquid and then purify and remove impurities to obtain an alkaline zinc-containing liquid purification liquid, which is alkaline zinc-containing liquid, for subsequent use; the above-mentioned acidic zinc-containing liquid Mix with the alkaline zinc-containing solution obtained above in a ratio of 1:1 for reaction, filter the obtained liquid after the reaction, wash the obtained filter cake with water for 2 to 3 times, dry at 140°C for 0.8h, and obtain zinc hydroxide , and then dissolve the zinc hydroxide with an excessive amount ...