Manufacturing method for environmental friendly thermal insulation material used in low-temperature pipe
A technology for thermal insulation materials and production methods, which is applied to building thermal insulation materials, building components, non-woven fabrics, etc., which can solve the problems of high cost of thermal insulation materials and achieve moderate strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Embodiment 1: the acidic solution is a 5% hydrochloric acid solution, and the soaking time is 5 minutes.
[0024] The raw materials required in asphalt modification treatment include 80 parts of pitch, 2 parts of stabilizer, 10 parts of polyethylene, 5 parts of aromatic oil, 20 parts of epoxy resin, 3 parts of titanium dioxide, 1 part of prooxidant, 4 parts of starch components.
[0025] The asphalt modification method is as follows: react asphalt, polyethylene, and epoxy resin at a temperature of 150°C and air-air oxidation for 5 hours, then add aromatic oil, pro-oxidant and starch, and raise the temperature to 300°C , followed by air blowing oxidation for 1 hour, then take it out and knead with stabilizer and titanium dioxide in a kneader for 10 minutes, then take it out.
Embodiment 2
[0026] Embodiment 2: the acidic solution is 6% hydrochloric acid solution, and the soaking time is 10 minutes.
[0027] The raw materials required in asphalt modification treatment include 90 parts of pitch, 5 parts of stabilizer, 15 parts of polyethylene, 8 parts of aromatic oil, 25 parts of epoxy resin, 6 parts of titanium dioxide, 2 parts of prooxidant, 7 parts of starch components.
[0028] The asphalt modification treatment method is: react asphalt, polyethylene, and epoxy resin at a temperature of 200°C and air-air oxidation for 8 hours, then add aromatic oil, pro-oxidant and starch, and raise the temperature to 350°C , followed by air blowing oxidation for 3 hours, then take it out and knead with stabilizer and titanium dioxide in a kneader for 20 minutes, then take it out.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap