A waterproof, mildew-proof, glue-coating technology, which is applied in the direction of anti-fouling/underwater coatings, coatings, adhesives, etc., can solve the problems of large limitations, unusability, single glue-coating function, etc., and achieve good use effect and simple production Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0007] 40 parts of isopropyl acrylate, 12 parts of epoxy resin, 40 parts of ethylene glycol monopropyl ether, 20 parts of ethyl acrylate, 12 parts of benzoyl peroxide, 10 parts of dibutyl phthalate, 8 parts of polyester 20 parts of butanediol acrylate, 4 parts of trimethylolpropane, 10 parts of butanediol, 10 parts of methoxyphenol, 8 parts of acrylamide, and 10 parts of styrene are put into the reactor, stirring continuously, mixing After completion, heat to 65°C, and react twice under a 200W / cm ultraviolet lamp at a speed of 16m / min to obtain the product.
Embodiment 2
[0009] 60 parts of isopropyl acrylate, 14 parts of epoxy resin, 45 parts of ethylene glycol monopropyl ether, 30 parts of ethyl acrylate, 18 parts of benzoyl peroxide, 15 parts of dibutyl phthalate, 12 parts of polyester 25 parts of butanediol acrylate, 5 parts of trimethylolpropane, 15 parts of butanediol, 15 parts of methoxyphenol, 10 parts of acrylamide, and 15 parts of styrene are put into the reactor, stirring constantly, mixing After completion, heat to 65°C, and react twice under a 200W / cm ultraviolet lamp at a speed of 16m / min to obtain the product.
Embodiment 3
[0011] 80 parts of isopropyl acrylate, 16 parts of epoxy resin, 50 parts of ethylene glycol monopropyl ether, 40 parts of ethyl acrylate, 24 parts of benzoyl peroxide, 20 parts of dibutyl phthalate, 16 parts of polyester 30 parts of butanediol acrylate, 6 parts of trimethylolpropane, 20 parts of butanediol, 10-20 parts of methoxyphenol, 12 parts of acrylamide, and 20 parts of styrene are put into the reactor and kept stirring , after mixing completely, heat to 65°C, and react twice under a 200W / cm ultraviolet lamp at a speed of 16m / min to obtain the product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com