Embodiment 1
[0070] The preparation of the color developer used as the hydrochromic covert writing liquid of the present invention.
[0071] Taking the color developer C12 as an example, its synthesis is as follows:
[0072] 1) Synthesis of intermediate nitroketo acid
[0073] Mix 2.95g (14.0mmol) 3-nitrophthalic anhydride and 2.50g (15.0mmol) N, N-diethyl-m-aminophenol evenly and add them to a 100mL single-necked bottle, then add 20mL toluene as a solvent , heated to reflux for 7 hours, the reaction was completed, cooled to room temperature to remove toluene under reduced pressure, dissolved with 25mL chloroform and transferred to a 100mL beaker, washed with 20mL (1N) dilute hydrochloric acid and then washed twice with 20mL water, extracted three times with 60mL saturated aqueous sodium carbonate solution, The aqueous phases were combined and acidified with hydrochloric acid to precipitate a pale yellow solid, which was suction filtered and the filter cake was washed with cold water unti...
Embodiment 2
[0077] Preparation of hydrochromic covert writing fluid.
[0078] The color developer, organic solvent, water and binder described in Example 1 are mixed and homogenized at a mass ratio of 0.0001-1:0-200:5-200:1-30 to obtain hydrochromic Covert writing fluid.
[0079] For different chromogenic agents, specific examples are as follows:
[0080] Use C12 as the developer, silane compound as the organic solvent, and polyethylene glycol as the binder: dissolve 20mg of C12 in 50ml of silane coupling agent, dissolve 20g of polyethylene glycol in 200mL of water, mix the two and use After the homogenizer disperses evenly, the hydrochromic covert writing solution is obtained. Dip the obtained hydrochromic recessive writing solution on the paper with a brush. After the water evaporates and dries up, the handwriting will not be visible. When the written position is treated with water, dark green handwriting will appear.
[0081] With C21 as the chromogenic layer and polyethylene glycol...
Embodiment 3
[0087] The hydrochromic invisible writing solution prepared in Example 2 is coated on the paper or board and dried to obtain reusable water writing paper or writing board. Use a brush or pen dipped in water to write on the surface of the above-mentioned reusable water-based writing paper or writing board, or use the above-mentioned water-based writing paper as the printing medium to print with water jets from an inkless printer, and then the writing or pattern can be displayed, and the writing will be displayed after the water evaporates and dries. Disappears, enabling reusability.
[0088] According to the needs of the use environment, one or more of the following performance-enhancing additives can also be added, such as humectants, anti-foaming agents, surfactants, antistatic agents, hardening agents, antistatic agents, antioxidants, preservatives or Leveling agent, etc.
[0089] The hydrochromic invisible writing liquid can also be coated on fibers, such as clothes or fab...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com