[0020] The present invention also provides a preparation method of nickel-plating brightener. 30-200 parts by weight of antimony potassium tartrate, 1-12 parts by weight of fatty amine, 4-12 parts by weight of naphthalene sulfonate, 2-15 parts by weight Parts of sodium bisulfite, 2-mercaptobenzimidazole of 4-15 parts by weight, polyethylene glycol of 6-14 parts by weight, lactic acid of 1-7 parts by weight and water of 30-200 parts by weight are mixed to obtain the Described nickel-plating brightener; Preferably, described nickel-plating brightener comprises the antimony potassium tartrate of 40-150 weight part, the fatty amine of 2-10 weight part, the naphthalene sulfonate of 6-10 weight part, 5-10 parts by weight of sodium bisulfite, 6-12 parts by weight of 2-mercaptobenzimidazole, 7-12 parts by weight of polyethylene glycol, 1-6 parts by weight of lactic acid and 50-100 parts by weight of water.
[0021] Aliphatic amines refer to a large class of organic amine compounds wit...
Embodiment 1
[0025] 30 parts by weight of potassium antimony tartrate, ethylenediamine of 1 part by weight, naphthalene sulfonate of 4 parts by weight, sodium bisulfite of 2 parts by weight, 2-mercaptobenzimidazole of 4 parts by weight, 6 parts by weight of The polyoxyethylene glycol 12000, the lactic acid of 1 weight part and the water of 30 weight parts are mixed, obtain nickel-plating brightener 1.
Embodiment 2
[0027] The antimony potassium tartrate of 200 parts by weight, the tetraethylenepentamine of 12 parts by weight, the naphthalene sulfonate of 12 parts by weight, the sodium bisulfite of 15 parts by weight, the 2-mercaptobenzimidazole of 15 parts by weight, 14 parts by weight Parts of polyethylene glycol 6000, 7 parts by weight of lactic acid, 5 parts by weight of sodium benzoate and 200 parts by weight of water are mixed to obtain brightener 2 for nickel plating.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com