A kind of preparation method of denim fabric
A technology for denim fabrics and dyes, applied in dyeing method, liquid/gas/vapor yarn/filament processing, textile and papermaking, etc., can solve the problems of low yield of denim fabrics, poor dyeing working environment, and substandard environmental protection. Achieve the effect of improving the coloring rate, no chromatic aberration, and great environmental protection pressure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036]This embodiment proposes a kind of preparation method of denim fabric, adopts cotton fiber to make described denim fabric after oxygen bleaching, dyeing, spinning, weaving, washing, and this dyeing comprises the following steps:
[0037] (1) Pretreatment: Make the cotton fiber after oxygen bleaching into a silk cake and put it into the dyeing vat, control the amount of cotton fiber and water according to the bath ratio of 1:5, and add additives to it;
[0038] (2) Dyeing: Add dye, sodium sulfate and alkali to the tank to dye the cotton fiber;
[0039] (3) Post-treatment: dyed cotton fibers are treated with oil to obtain dyed fiber products.
Embodiment 2
[0041] This embodiment proposes a kind of preparation method of denim fabric, adopts cotton fiber to make described denim fabric after oxygen bleaching, dyeing, spinning, weaving, washing, and this dyeing comprises the following steps:
[0042] (1) Pretreatment: make the cotton fiber after oxygen bleaching into a silk cake and put it into the dyeing vat, control the amount of the cotton fiber and water according to the bath ratio of 1:12, and add additives to it;
[0043] (2) Dyeing: Add dye, sodium sulfate and alkali to the tank to dye the cotton fiber;
[0044] (3) Post-treatment: dyed cotton fibers are treated with oil to obtain dyed fiber products.
Embodiment 3
[0046] This example proposes a preparation method of a denim fabric, which uses cotton fibers to undergo oxygen bleaching, dyeing, spinning, weaving, and washing to prepare the denim fabric.
[0047] In the above process, oxygen bleaching is to control the amount of cotton fiber and water according to the bath ratio of 1:6, and add hydrogen peroxide, hydrogen peroxide stabilizer, penetrant and scouring enzyme to it in order to control the concentration of hydrogen peroxide, hydrogen peroxide stabilizer and penetrant in the bath. The concentration of scouring enzyme and scouring enzyme is 26g / L, 1g / L, 1g / L, 1g / L in turn, heat to 85°C, keep warm for 60min, then add glacial acetic acid to it, after adding glacial acetic acid, the glacial acetic acid in the bath The concentration is 0.3g / L, the temperature is controlled at 30°C, and the temperature is kept for 50 minutes to complete the oxygen bleaching process.
[0048] Staining involves the following steps:
[0049] (1) Pretrea...
PUM
Property | Measurement | Unit |
---|---|---|
height | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com