A high-strength, heat-resistant technology, applied in the field of new energy and environmental protection and energy saving, can solve the problems of low electrical performance and water absorption, aging resistance, dimensional stability and processing performance, poor dimensional stability, and poor aging resistance. Achieve the effects of mass production, low cost, dimensional stability and remarkable processing performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] An efficient and environmentally friendly high-strength heat-resistant PBT-PP alloy, comprising the following parts by weight: the PBT is 75 parts by weight, the PP is 45 parts by weight, the glass fiber is 30 parts by weight, and the compatibilizer is 10 parts by weight, the dibutyl phthalate is 20 parts by weight, the benzylidene acetone is 15 parts by weight, the lubricant is 1.5 parts by weight, and the disulfide is 8 parts by weight.
Embodiment 2
[0020] An efficient and environmentally friendly high-strength heat-resistant PBT-PP alloy, comprising the following parts by weight: the PBT is 80 parts by weight, the PP is 50 parts by weight, the glass fiber is 35 parts by weight, and the compatibilizer is 13 parts by weight, the dibutyl phthalate is 23 parts by weight, the benzylidene acetone is 18 parts by weight, the lubricant is 1.8 parts by weight, and the disulfide is 10 parts by weight.
Embodiment 3
[0022] An efficient and environmentally friendly high-strength heat-resistant PBT-PP alloy, comprising the following parts by weight: the PBT is 90 parts by weight, the PP is 60 parts by weight, the glass fiber is 45 parts by weight, and the compatibilizer is 15 parts by weight, the dibutyl phthalate is 25 parts by weight, the benzylidene acetone is 20 parts by weight, the lubricant is 2 parts by weight, and the disulfide is 15 parts by weight. Wherein, the intrinsic viscosity of the PBT is 0.8-1.3dl / g, and the compatibilizer is EVA and / or EVA-g-MAH, the PBT and the compatibilizer of the above content can better increase the overall high strength The mechanical properties of the heat-resistant PBT-PP alloy, the glossiness of the surface of the high-strength heat-resistant PBT-PP alloy can be improved by adding benzylidene acetone.