Sizing process of pine needle velvet fabric yarns
A fleece fabric and yarn technology, applied in the field of sizing technology, can solve problems such as performance to be improved, and achieve the effects of improved strength, yarn hairiness, and good elongation retention performance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of pine needle fleece yarn comprises the steps:
[0026] 1) 1 to 2 parts by weight of diethyl carbonate, 1.8 parts by weight of triethanolamine oleate, 1.3 parts by weight of polyacrylate, 0.8 parts by weight of γ-glycidyl ether trimethoxysilane, 11 parts by weight of polyethylene Alcohol is dropped into 25 parts by weight of deionized water successively and stirred evenly;
[0027] 2) then drop into 0.7 parts by weight of sodium oleoyl amino acid, 1.1 parts by weight of isomeric tridecanol polyoxyethylene ether phosphate, 0.5 parts by weight of sodium petroleum sulfonate, and 1.3 parts by weight of dimethyl diallyl ammonium chloride, Continue to stir until fully mixed to obtain a slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of pine needle fleece yarn comprises the steps:
[0031] 1) 1 part by weight of diethyl carbonate, 1.8 parts by weight of triethanolamine oleate, 1.3 parts by weight of polyacrylate, 0.8 parts by weight of γ-glycidyl ether trimethoxysilane, and 11 parts by weight of polyvinyl alcohol Drop into 25 parts by weight of deionized water and stir evenly;
[0032] 2) then drop into 0.7 parts by weight of sodium oleoyl amino acid, 1.1 parts by weight of isomeric tridecanol polyoxyethylene ether phosphate, 0.5 parts by weight of sodium petroleum sulfonate, and 1.3 parts by weight of dimethyl diallyl ammonium chloride, Continue to stir until fully mixed to obtain a slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of pine needle fleece yarn comprises the steps:
[0036] 1) 2 parts by weight of diethyl carbonate, 1.8 parts by weight of triethanolamine oleate, 1.3 parts by weight of polyacrylate, 0.8 parts by weight of γ-glycidyl ether trimethoxysilane, and 11 parts by weight of polyvinyl alcohol Drop into 25 parts by weight of deionized water and stir evenly;
[0037] 2) then drop into 0.7 parts by weight of sodium oleoyl amino acid, 1.1 parts by weight of isomeric tridecanol polyoxyethylene ether phosphate, 0.5 parts by weight of sodium petroleum sulfonate, and 1.3 parts by weight of dimethyl diallyl ammonium chloride, Continue to stir until fully mixed to obtain a slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com