A bamboo pulp and paper pulp technology, applied in the field of pulping and papermaking, can solve the problems of tensile strength, softness, water absorption not meeting the specified standards, fiber strength damage, strength and toughness decline, etc., to avoid possible damage to the human body. The effect of damage, elimination of residual pollution, and low consumption of raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] The preparation of Cizhu pulp, it comprises the following steps:
[0028] S1. Raw material disintegration: choose Moso bamboo, yellow bamboo and Ci bamboo as raw materials, and dry the raw materials into bamboo pieces with a length of 2 cm;
[0029] S2. Cooking: Soak the bamboo slices with the cooking liquid, the soaking time is 50min, the temperature of the soaking liquid is 85°C, mix the bamboo slices and the cooking liquid evenly at a material-to-liquid ratio of 1:2.5, and then add them to the ball digester. Pass in steam to heat up to 125°C, heat up, let out a little air, and keep warm for 60 minutes to obtain a high-hardness pulp with a hardness of potassium permanganate value 40; the cooking liquid is 10% NaOH;
[0030] S3. Thinning: the above-mentioned high-hardness pulp is sent to the high-consistency refiner for thinning, and the thinning time is 25 minutes;
[0031] S4. Refining: dilute the bamboo pulp after thawing with dilute black liquor to a concentration...
Embodiment 2
[0034] The preparation of Cizhu pulp, it comprises the following steps:
[0035] S1. Raw material disintegration: choose water bamboo and white acacia as raw materials, and dry the raw materials into bamboo pieces with a length of 4 cm;
[0036] S2. Cooking: Mix bamboo slices and cooking liquid evenly at a material-to-liquid ratio of 1:4, and then continue the digester, feed steam to heat up to 140°C, heat up, deflate, and keep warm for 70 minutes, and the hardness is potassium permanganate The high hardness pulp of value 30; Wherein, described cooking liquid is the NaOH of 17%;
[0037] S3. Thinning: the above-mentioned high-hardness pulp is sent to the high-consistency refiner for thinning, and the thinning time is 30 minutes;
[0038] S4. Refining: dilute the bamboo pulp after diluting with dilute black liquor to a concentration of 10%, and refine the diluted pulp to obtain a pulp with a beating degree of 28 ° SR;
[0039] S5. Screening and washing: screen the pulp after ...
Embodiment 3
[0041] The preparation of Cizhu pulp, it comprises the following steps:
[0042] S1. Raw material disintegration: choose Xifeng Cizhu as raw material, and dry disintegrate the raw material into bamboo chips with a length of 3 cm;
[0043] S2. Cooking: Soak the bamboo slices with the cooking liquid, the soaking time is 60min, the temperature of the soaking liquid is 90°C, put the bamboo slices into the cooking pot from the hot black liquor through the pot loader, and close the pot when it is full Cover the pot, add cooking liquid at a temperature of 100°C to the cooking pot, and at the same time discharge the air in the pot and raise the pressure to 0.2MPa, heat up the cooking liquid to 125°C, heat up, keep warm and replace for 70 minutes, and finally use the conveying screw to release the slurry to To spray pot, get the high hardness pulp that hardness is potassium permanganate value 35; Wherein, described cooking liquid is the NaOH of 13%, and the add-on of bamboo chips and c...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
length | aaaaa | aaaaa |
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com