Negative pressure drainage device used for wound repairing
A negative pressure drainage and wound repair technology, applied in the field of medical devices, can solve problems such as poor drainage of sponges, easily blocked sponges, unusable medical sponges, etc., to reduce scar generation, prevent wound drying, and have good absorption and exudation ability. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Sodium carboxymethyl cellulose, sodium polyacrylate, and water-soluble chitosan with a weight ratio of 5:3:11 were dissolved in deionized water to prepare a spinning solution with a weight percentage of water-soluble chitosan of 5%, and ultrasonically 1h, adjust the spinning voltage to 30kV, the flow rate of the spinning solution to 1ml / h, cover the collecting cylinder with calcium alginate fibers, the distance between the calcium alginate fibers and the spinneret is 15cm, and the calcium alginate fibers are collected and spun immediately It is the polymer dressing layer.
Embodiment 2
[0025] Sodium carboxymethyl cellulose, sodium polyacrylate, and water-soluble chitosan with a weight ratio of 4:2:3 were dissolved in deionized water to prepare a spinning solution with a weight percentage of water-soluble chitosan of 8%, and ultrasonically 1h, adjust the spinning voltage to 25kV, the spinning liquid flow rate to 0.5ml / h, cover the collection cylinder with calcium alginate fibers, the distance between the calcium alginate fibers and the spinneret is 10cm, and the calcium alginate fibers are collected and spun It is the polymer dressing layer.
Embodiment 3
[0027] Sodium carboxymethyl cellulose, sodium polyacrylate, and water-soluble chitosan with a weight ratio of 6:1:8 were dissolved in deionized water to prepare a spinning solution with a weight percentage of water-soluble chitosan of 3%, and ultrasonically 1h, adjust the spinning voltage to 15kV, the flow rate of the spinning solution to 2ml / h, cover the collecting cylinder with calcium alginate fibers, the distance between the calcium alginate fibers and the spinneret is 12cm, and the calcium alginate fibers are collected and spun immediately It is the polymer dressing layer.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 