Manufacturing method of bobbin paper
A manufacturing method and bobbin paper technology are applied in the field of papermaking with waste paper, which can solve the problems of poor product quality, inability to meet usage requirements, and reduced production of recycled paper, achieving sufficient raw materials, saving raw materials and production steps, and stable quality. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] Crush the mature corn stalks and mix them with distiller's grains at a mass ratio of 1:1, add water to dilute to a concentration of 11%, then add compound mold with a mixed liquid quality of 1‰, ferment and hydrolyze for 40 minutes at room temperature to obtain fermented The mixed liquid after fermentation, wherein the upper layer of the fermented mixed liquid is lignin, the middle layer is semi-fiber, and the lower layer is fiber with a fiber length between 0.55 and 1.45 mm. The fibers in the lower layer are removed and cleaned, and dehydrated until the water content is 70% to 80%. in between.
[0034] Take 400kg of fiber pulp obtained through the above treatment and 600kg of waste paper pulp and mix them uniformly at a ratio of 4:6, add water to dilute to a concentration of 1-1.5%, add 4kg of reinforcing agent polyvinyl alcohol, 4kg of waterproofing agent AKD, and adhesive 4kg of polyacrylamide, 12kg of preservative, and 24kg of stone powder, after mixing and stirring...
Embodiment 2
[0036] Grind mature corn stalks and mix them with distiller's grains at a mass ratio of 1:1, add water to dilute to a concentration of 25%, then add compound mold with a mixed liquid quality of 1.5‰, ferment and hydrolyze at room temperature for 50 minutes, and obtain fermented The mixed liquid after fermentation, wherein the upper layer of the fermented mixed liquid is lignin, the middle layer is semi-fiber, and the lower layer is fiber with a fiber length between 0.55 and 1.45 mm. The fibers in the lower layer are removed and cleaned, and dehydrated until the water content is 70% to 80%. in between. .
[0037] Take 200kg of the fiber pulp obtained through the above treatment and 800kg of waste paper pulp and mix them uniformly at a ratio of 2:8, add water to dilute to a concentration of 1.5-2%, add in turn 10kg of reinforcing agent polyvinyl alcohol, 10kg of waterproofing agent AKD, and adhesive 30kg of polyacrylamide, 15kg of preservative, and 30kg of stone powder, after m...
Embodiment 3
[0039]Crush the mature corn stalks and mix them with distiller's grains at a mass ratio of 1:1, add water to dilute to a concentration of 15%, then add compound mold with a mixed liquid quality of 1.2‰, ferment and hydrolyze at room temperature for 45 minutes to obtain fermented The mixed liquid after fermentation, wherein the upper layer of the fermented mixed liquid is lignin, the middle layer is semi-fiber, and the lower layer is fiber with a fiber length between 0.55 and 1.45 mm. The fibers in the lower layer are removed and cleaned, and dehydrated until the water content is 70% to 80%. in between.
[0040] Take 300kg of fiber pulp obtained through the above treatment and 700kg of waste paper pulp and mix them uniformly at a ratio of 3:7, add water to dilute to a concentration of 1.3-2%, add 10kg of reinforcing agent polyvinyl alcohol, 10kg of waterproofing agent AKD, and adhesive 30kg of polyacrylamide, 15kg of preservative, and 30kg of stone powder, after mixing and stir...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com