Bubble bag material
A bubble bag and plastic technology, applied in the field of materials, can solve the problems of high preparation cost, high raw material requirements, blow molding, sealing, weather resistance and environmental protection, etc., and achieve the effect of improving heat resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The components of the bubble bag material of the present invention are calculated in parts by weight: 32 parts of low-density polyethylene plastic particles, 15 parts of acetyl citrate, 8 parts of plastic deodorant, 12 parts of pineapple extract, and 5 parts of citronella extract , Surface active agent 5 parts, paraffin wax 10 parts, 7 parts dicumyl peroxide.
[0016] The preparation method of the bubble bag material is: first dry the low-density polyethylene plastic particles, then heat to a liquid state, remove water through a reduced pressure evaporator, and then add acetyl citrate, paraffin wax and diisopropyl peroxide Stir the benzene evenly, heat it to 33°C again, add the remaining components and mix them together to obtain the bubble bag material.
Embodiment 2
[0018] The components of the bubble bag material of the present invention are calculated in parts by weight: 30 parts of low-density polyethylene plastic particles, 16 parts of acetyl citrate, 7 parts of plastic deodorant, 14 parts of pineapple extract, 12 parts of citronella extract , 7 parts of surfactants, 8 parts of paraffin, 10 parts of dicumyl peroxide.
[0019] The preparation method of the bubble bag material is: first dry the low-density polyethylene plastic particles, then heat to a liquid state, remove water through a reduced pressure evaporator, and then add acetyl citrate, paraffin wax and diisopropyl peroxide Stir the benzene evenly, heat it to 38°C again, add the remaining components and mix them together to obtain the bubble bag material.
Embodiment 3
[0021] The components of the bubble bag material of the present invention are calculated in parts by weight: 40 parts of low-density polyethylene plastic particles, 18 parts of acetyl citrate, 10 parts of plastic deodorant, 16 parts of pineapple extract, 9 parts of citronella extract , 8 parts of surface active agent, 13 parts of paraffin wax, 13 parts of dicumyl peroxide.
[0022] The preparation method of the bubble bag material is: first dry the low-density polyethylene plastic particles, then heat to a liquid state, remove water through a reduced pressure evaporator, and then add acetyl citrate, paraffin wax and diisopropyl peroxide Stir the benzene evenly, heat it to 32°C again, add the remaining components and mix them together to obtain the bubble bag material.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com