A technology of process flow and skirting line, which is applied in the field of new plastic-wood combined skirting line and its production process, can solve the problems of easy color difference, unfavorable human health, and non-waterproof skirting line, so as to reduce the contact area, Better shaping effect and strong structural firmness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] Example 1: See figure 1 As shown, it is a structural schematic diagram of a preferred embodiment of the present invention, a new plastic-wood combined skirting line, mainly including: a bottom layer 1, a surface layer 4 and a medium layer 3, and the first three surfaces of the bottom layer 1 are up and down. Covered by the surface layer 4, the bottom layer 1 and the surface layer 4 are combined through the medium layer 3. When processing the new plastic-wood combined skirting line, the top three surfaces of the bottom layer 1 are covered with the surface layer 4, and the three breads are covered. Relative to the two sides, the structure is stronger, and the three breads are opposed to the four sides, and the substances in the material of the bottom layer 1 can be released through the uncoated back, and the air permeability is better.
[0040] The bottom layer 1 is solid wood, and the environmental protection of the solid wood material is superior to other materials. The...
Embodiment 2
[0044] Example 2: See Figure 1~3 As shown, it is a schematic structural diagram of a preferred embodiment of the present invention, a production process of a new plastic-wood combined skirting line, including the following steps:
[0045] ①Substrate surface treatment: Apply filler 2 on the upper, lower, front, and rear surfaces of the solid wood base layer 1 to fill and reinforce the solid wood surface to improve the performance of the material, and then apply plastic-wood adhesive on the upper, lower, and front three surfaces of the solid wood base layer 1 , Plastic-wood adhesive can make the extruded plastic and the solid wood surface tightly bonded;
[0046] ②Plastic machine start-up and heating: Turn on the power of the plastic machine, control the temperature of the heating zone to rise, and when the temperature reaches a certain value, put plastic particles into the heating zone, and the plastic particles flow out of the funnel bin and enter the heating zone to melt;
...