A sleep quality and production method technology, applied in the manufacture of tools, peeling of wicker poles, reed/straw treatment, etc., can solve the problems of unreasonable and unscientific production methods, poor sleep quality of middle-aged and elderly people, and failure to improve sleep quality. The production method is scientific and reasonable, the peeling work is easy, and the effect of increasing the time of deep sleep
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A method for making a wicker deck chair that can improve sleep quality includes the following steps:
[0026] (1) Harvest wicker with uniform thickness and disease-free pests in the early morning on a sunny day, and dry it flat until the leaves are dry, and when the water content of the leaves is less than 3%, remove the dry leaves;
[0027] (2) Wash the leaves of the wicker with clean water to remove impurities, and then soak it in the pretreatment solution for two hours, peel off the willow bark after taking it out, and rinse it with clean water;
[0028] (3) Dry the wicker treated in step (2) with hot air at 50 degrees Celsius until the moisture content of the wicker is less than 20%;
[0029] (4) Soak the dried wicker in a mixed reagent at 60 degrees Celsius for 4 hours, and then wash it with water;
[0030] (5) Use the cleaned wicker and stainless steel frame in step (4) to weave into a recliner;
[0031] (6) Dry the woven recliner with hot air at 60 degrees Celsius until the...
Embodiment 2
[0036] A method for making a wicker deck chair that can improve sleep quality includes the following steps:
[0037] (1) Harvest wicker with uniform thickness and no pests and diseases in the early morning on a sunny day, and dry it flat until the leaves are dry, and when the water content of the leaves is less than 3%, remove the dry leaves;
[0038] (2) Wash the wicker leaves with clean water to remove impurities, and then soak it in the pretreatment solution for two hours, remove the willow bark, and rinse it with clean water;
[0039] (3) Dry the wicker treated in step (2) with hot air at 40 degrees Celsius until the moisture content of the wicker is lower than 20%;
[0040] (4) Soak the dried wicker in a mixed reagent at 50 degrees Celsius for 4 hours, and then wash it with water;
[0041] (5) Use the cleaned wicker and stainless steel frame in step (4) to weave into a recliner;
[0042] (6) Dry the woven recliner with hot air at 60 degrees Celsius until the moisture content is less...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com