Inside surface plastic-coated steel pipeline crater anticorrosion treatment method

An anti-corrosion treatment and pipeline technology, applied in the direction of coating, etc., can solve the problems of internal plastic-coated welded pipeline anti-corrosion and other problems, and achieve the effect of ensuring anti-corrosion performance and water quality

Inactive Publication Date: 2018-02-16
BEIJING SHOUGANG CONSTR GROUP
View PDF8 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The purpose of the present invention is to provide a method for anti-corrosion treatment of plastic-coated steel pipe weld joints, which solves the internal anti-corrosion problem of plastic-coated welded pipes, and uses the waste heat during welding to internally coat the weld joints of the pipes with a PE anti-corrosion layer to ensure that the pipes are protected against corrosion. Internal corrosion protection at the weld

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Inside surface plastic-coated steel pipeline crater anticorrosion treatment method

Examples

Experimental program
Comparison scheme
Effect test

Embodiment approach

[0018] 1. Pipe cutting:

[0019] The length of the inner plastic-coated pipe is determined according to the site conditions, and the length of the stainless steel nipple is determined according to the diameter of the inner plastic-coated pipe. The general length is 250mm. The smoothness also protects the inner plastic anti-corrosion layer from being damaged.

[0020] 2. Grinding of nozzle and treatment of anti-corrosion layer

[0021] After the pipe cutting is completed, in order to ensure the welding quality, the inner plastic-coated pipe and the stainless steel pipe mouth should be grooved to remove the burrs of the pipe mouth, and the PE coating in the inner plastic-coated pipe should be cut and scraped to make it weldable during welding. don't get hurt. Generally cut and scrape 30mm.

[0022] 3. Butt connection between stainless steel pup joint and steel pipe:

[0023] According to the requirements of the drawing, when the stainless steel pup joint is aligned with the ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses an inside surface plastic-coated steel pipeline crater anticorrosion treatment method and belongs to the technical field of pipeline connection construction crater anticorrosion. The method comprises the following construction steps of blanking cutting of an inside surface plastic-coated pipeline and a stainless steel pipe section; polishing of a pipe orifice and treatmentof an anticorrosive layer; assembling of pipelines; welding of the pipelines; and anticorrosion treatment of a crater. In order to ensure the welding quality and the anticorrosive layer of the craterand a welding seam, the pipe orifice needs to be subjected to groove polishing and anticorrosive layer treatment, and the anticorrosive layer in the inside surface plastic-coated pipeline is cut and scraped off at the same time, so that the inside surface plastic-coated pipeline cannot deform caused by welding and being heated; and the welding process needs to be continuously performed, after welding of the pipeline crater is finished, the welding seam is cleaned, PE powder is coated and scattered and is melted by utilizing residual heat produced during pipeline welding, and the welded pipeline is rotated to form a layer of uniform PE anticorrosive layer. The inside surface plastic-coated steel pipeline crater anticorrosion treatment method is mainly suitable for connection of inside surface plastic-coated PE composite pipes and adopts effective transition connection with addition of a stainless steel short section under the condition that a fixed length of the pipeline is not satisfied, so that the PE anticorrosive layer is ensured to form at the crate on the inner wall of the pipeline, and the anticorrosion performance and the water quality of the pipeline are strongly guaranteed.

Description

technical field [0001] The invention belongs to the technical field of pipeline installation and construction, and in particular provides a method for anti-corrosion treatment of plastic-coated steel pipeline welding joints. The material PE is used for anti-corrosion treatment of pipeline welds, which is suitable for the welding of plastic-coated steel pipelines after welding. The construction of anti-corrosion treatment engineering can improve the anti-corrosion ability of the inner wall of the pipeline after anti-corrosion treatment, prevent secondary pollution of water bodies, and thus meet the requirements of water quality standards. Background technique [0002] In pipeline construction, the anti-corrosion treatment inside the weld seam is a difficult problem that is often encountered. There are stainless steel short joints attached to both ends of the plastic-coated steel pipes. After the manufacturer has cut and shaped them, they will be cut and blanked during the ins...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine