Preparation method of waterproof corrugated packaging carton
A water-resistant, corrugated paper technology, applied in packaging, transportation and packaging, rigid/semi-rigid container manufacturing, etc., can solve problems such as poor water resistance, and achieve the effect of improving water resistance and moisture resistance, and good water resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A method for preparing a water-resistant corrugated packaging carton, comprising the steps of:
[0023] S1, the pulverization of coating, take 10 parts of thermosetting polymer, thermosetting polymer is one of allyl propylene polymer, phenolic resin and epoxy resin, then take 10 parts of petroleum wax and put it into a pulverizer to pulverize into powder, put the two items into the mixing device for thorough mixing;
[0024] S2. Preparation of paint. Put the powder mixed in S1 into a heating furnace to heat and stir. When the powder is in a molten state, stop heating and keep warm. The heating temperature is 66°C, which is higher than the melting point of petroleum wax and lower than that of thermosetting polymerization. solidification temperature, so that the thermosetting polymer is evenly and fully dispersed in the molten petroleum wax, and a small amount of antioxidant is added when melting;
[0025] S3, cardboard coating, take the surface layer of fiber paper and ...
Embodiment 2
[0031] A method for preparing a water-resistant corrugated packaging carton, comprising the steps of:
[0032] S1, the pulverization of coating, take 20 parts of thermosetting polymer, thermosetting polymer is one of allyl propylene polymer, phenolic resin and epoxy resin, then take 20 parts of petroleum wax and put it into a pulverizer to pulverize into powder, put the two items into the mixing device for thorough mixing;
[0033] S2. Preparation of paint. Put the powder mixed in S1 into a heating furnace to heat and stir. When the powder is in a molten state, stop heating and keep warm. The heating temperature is 67°C, which is higher than the melting point of petroleum wax and lower than that of thermosetting polymerization. solidification temperature, so that the thermosetting polymer is evenly and fully dispersed in the molten petroleum wax, and a small amount of antioxidant is added when melting;
[0034] S3, cardboard coating, take the surface layer of fiber paper and ...
Embodiment 3
[0040] A method for preparing a water-resistant corrugated packaging carton, comprising the steps of:
[0041] S1, pulverization of coating, take 30 parts of thermosetting polymer, thermosetting polymer is one of allyl propylene polymer, phenolic resin and epoxy resin, then take 30 parts of petroleum wax and put it into a pulverizer for pulverization into powder, put the two items into the mixing device for thorough mixing;
[0042] S2, preparation of paint, put the powder mixed in S1 into a heating furnace to heat and stir, stop heating and keep warm when the powder is in a molten state, the heating temperature is 68°C, which is higher than the melting point of petroleum wax and lower than that of thermosetting polymerization solidification temperature, so that the thermosetting polymer is evenly and fully dispersed in the molten petroleum wax, and a small amount of antioxidant is added when melting;
[0043] S3, cardboard coating, take the surface layer of fiber paper and s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com