Application of potassium persulfate in preparing potassium monopersulfate compound salt and preparation method of potassium monopersulfate compound salt
A technology of potassium monopersulfate and potassium peroxodisulfate, which is applied in the field of preparation of inorganic peroxides, can solve the problems of complex preparation process and difficulty in meeting the product quality requirements of potassium monopersulfate compound salt, and achieve simple production process , shorten the preparation time, reduce the effect of the preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0042] A kind of preparation method of potassium monopersulfate compound salt:
[0043] In step a, add 61g of 70wt% hydrogen peroxide into a 1000ml four-neck flask with stirring and a thermometer, and use a low-temperature thermostat to control the temperature so that the system temperature reaches -2°C. 215g of 65wt% fuming sulfuric acid was added dropwise to the container, and the dropwise addition time was 2h, and the temperature was kept for 25min to obtain the peroxidation reaction solution;
[0044] Step b, control the temperature in the reactor to 18°C, add dropwise 300g of the crystallization dehydration mother liquor containing 1wt% potassium peroxodisulfate to the peroxidation reaction solution, and add the dropwise time for 25min, then control the temperature at 23°C, add Potassium bicarbonate 250g, the addition time is controlled to be 120min, obtains the neutralization reaction liquid;
[0045] In step c, the neutralization reaction liquid is cooled to -8°C to cr...
Embodiment 2
[0047] A kind of preparation method of potassium monopersulfate compound salt:
[0048] In step a, add 105g of 65wt% hydrogen peroxide into a 1000ml four-necked flask with stirring and a thermometer, and use a low-temperature thermostat to control the temperature so that the system temperature reaches 0°C. Add 230g of 30wt% oleum dropwise for 2.5 hours, and keep warm for 30 minutes to obtain a peroxidation reaction solution;
[0049] Step b, control the temperature in the reactor to 20°C, add dropwise 368g of crystallization dehydration mother liquor containing 5wt% potassium peroxodisulfate to the peroxidation reaction solution, the dropping time is 15min, then control the temperature at 25°C, add Potassium bicarbonate 300g, the addition time is controlled as 60min, to obtain the neutralization reaction solution;
[0050] Step c, the neutralization reaction solution is cooled to -2°C to crystallize, the crystallization time is 90min, centrifuged, and dried at 60°C to obtain ...
Embodiment 3
[0052] A kind of preparation method of potassium monopersulfate compound salt:
[0053] In step a, add 142g of 60wt% hydrogen peroxide into a 1000ml four-necked flask with stirring and a thermometer, and use a low-temperature thermostat to control the temperature so that the system temperature reaches 5°C. 240g of 10wt% fuming sulfuric acid was added dropwise for 3 hours and kept for 35 minutes to obtain a peroxidation reaction solution;
[0054] Step b, control the temperature in the reactor to 22°C, add dropwise 380g of crystallization dehydration mother liquor containing 10wt% potassium peroxodisulfate to the peroxidation reaction solution, the dropping time is 5min, then control the temperature at 27°C, add Potassium bicarbonate 350g, the addition time is controlled to be 20min, obtains the neutralization reaction liquid;
[0055] Step c, the neutralization reaction solution is cooled to 5°C to crystallize, the crystallization time is 120min, centrifuged, and dried at 80°...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com