Repair glue for mineral water barrel and preparation method thereof

A mineral water bucket and repair glue technology, which is applied in the field of mineral water repair glue and its preparation, can solve the problems of high brittleness, low bonding strength, and easy breakage, and achieve the goals of increasing viscosity, increasing strength, and enhancing bonding strength and toughness Effect

Inactive Publication Date: 2018-12-11
QUZHOU DONGKAI GLUE IND CO LTD
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] At present, because there are too many damaged mineral water barrels in the water factory, it is often impossible to use the mineral water barrels if only a crack is broken, and the waste is particularly large; therefore, the factory is eager to have a method of repairing the mineral water barrels, so that the repaired barrels can be used repeatedly and save energy. energy, and will not pollute the environment
[0003] At present, there is no professional glue for repairing mineral water buckets in the market. Some of them are repaired with epoxy glue, but the effect is very poor.
Because epoxy glue has high hardness, high brittleness and easy to break, it is not suitable for use
The common all-purpose glue in the prior art is used to repair, but the effect is not good, the all-purpose glue is too soft, the bonding strength is low, the color is yellow, and the repaired wound is not beautiful

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Repair glue for mineral water barrel and preparation method thereof
  • Repair glue for mineral water barrel and preparation method thereof
  • Repair glue for mineral water barrel and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0039] 1) Get 49% by weight of the solvent and pour it into the reactor, then get 10% by weight of the SBS styrene-butadiene rubber particles and put it into the reactor, then put 6% by weight of the ABS resin into the reactor, and stir for 3 hours After the SBS styrene-butadiene rubber in the reactor is completely dissolved, add 4% by weight of PC polycarbonate resin, 20% by weight of hydrogenated petroleum resin, 1% by weight of white carbon black, 0.2% by weight of antioxidant agent, stirred for 1.5 hours until all the resins were dissolved;

[0040] 2) filling, take the ointment filling made in step 1).

[0041] The solvent is a mixture of methyl acetate, tetrahydrofuran, acetone and toluene.

[0042] The preparation method of the solvent: 20% by weight of methyl acetate, 8% by weight of tetrahydrofuran, 7% by weight of acetone and 4% by weight of toluene are added into a mixing vessel for mixing.

Embodiment 2

[0044] 1) Get 61% by weight of the solvent and pour it into the reactor, then get 20% by weight of the SBS styrene-butadiene rubber particles and drop it into the reactor, then put 10% by weight of the ABS resin into the reactor, stir for 5 hours, After the SBS styrene-butadiene rubber in the reaction kettle is completely dissolved, add 6% by weight of PC polycarbonate resin, 30% by weight of hydrogenated petroleum resin, 3% by weight of white carbon black, 0.4% by weight of antioxidant , stirred for 3 hours, and the resin was completely dissolved;

[0045] 2) filling, take the ointment filling made in step 1).

[0046] The solvent is a mixture of methyl acetate, tetrahydrofuran, acetone and toluene.

[0047] The preparation method of the solvent: take 30% by weight of methyl acetate, 12% by weight of tetrahydrofuran, 11% by weight of acetone and 8% by weight of toluene into a mixing vessel for mixing.

Embodiment 3

[0049] 1) Get 56% by weight of the solvent and pour it into the reactor, then get 15% by weight of the SBS styrene-butadiene rubber particles and drop it into the reactor, then put 8% by weight of the ABS resin into the reactor, stir for 2 hours, After the SBS styrene-butadiene rubber in the reactor is completely dissolved, add 5% by weight of PC polycarbonate resin, 25% by weight of hydrogenated petroleum resin, 2% by weight of white carbon black, 0.3% by weight of antioxidant , and stirred for 2 hours until the resin was completely dissolved;

[0050] 2) filling, take the ointment filling made in step 1).

[0051] The solvent is a mixture of methyl acetate, tetrahydrofuran, acetone and toluene.

[0052] The preparation method of the solvent: add 25% by weight of methyl acetate, 10% by weight of tetrahydrofuran, 10% by weight of acetone and 6% by weight of toluene into a mixing vessel for mixing.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a repair glue for a mineral water barrel. The repair glue is prepared from the following components of 6 to 10% of ABS (acrylonitrile butadiene styrene) resin, 20 to 30% of hydrocarbon-pentapentane petroleum resin, 1 to 3% of white carbon black, 10 to 20% of SBS (styrene butadiene styrene) styrene butadiene rubber, 0.2 to 0.4% of antioxidant, 4 to 6% of polycarbonate resin,and 49 to 61% of solvent. The repair glue has the advantages that the safe effect is realized, and the hidden hazard of health is avoided; after repairing, the sticking strength and toughness of thescratch part are enhanced; when the crack of the mineral water barrel is repaired, the linkage property and sticking strength are realized; the hardness after sticking is improved, and the cohesion force of the formula structure is improved; the viscosity is improved, the strength after crack sticking is improved, and the antioxidant reaches the anti-aging function.

Description

technical field [0001] The invention relates to the field of repair glue, more specifically, a mineral water repair glue and a preparation method thereof. Background technique [0002] At present, because there are too many damaged mineral water barrels in the water factory, it is often impossible to use the mineral water barrels if only a crack is broken, and the waste is particularly large; therefore, the factory is eager to have a method of repairing the mineral water barrels, so that the repaired barrels can be used repeatedly and save energy. energy and will not pollute the environment. [0003] At present, there is no professional glue for repairing mineral water buckets in the market. Some of them are repaired with epoxy glue, but the effect is very poor. Because epoxy glue has high hardness and high brittleness, it is not suitable for use. Adopt common all-purpose glue to repair in the prior art, but effect is also bad, and all-purpose glue is too soft, bonding str...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More