Biomass granular fuel combustion improver
A technology of biomass particles and combustion aids, which is applied in fuel, solid fuel, petroleum industry, etc. It can solve the problems of low ash melting point, affecting the combustion of biomass particle fuel, melting slagging, etc., and achieve the effect of enhancing the bonding strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A biomass particle fuel combustion accelerant, which is composed of the following raw materials in parts by weight: 50 parts of rice husk, 30 parts of kaolin, 20 parts of diatomite powder, 2 parts of iron oxide, 4 parts of quicklime, and 10 parts of cubic stone powder.
[0016] The rice husk is specifically the rice husk dried by a dryer, and the moisture content of the rice husk is 6%.
[0017] The diatomite powder is obtained by the following method: crush the diatomite through a crusher, put the broken diatomite block into a grinder for grinding, and pass the ground diatomite powder through a 80-mesh sieve .
[0018] The above mentioned method is obtained by the following method: crushing the square stone through a crusher, putting the crushed square stone into a grinder for grinding, and passing the ground square stone powder through a 150-mesh sieve .
[0019] The plasticity of the kaolin is: strong plasticity>153.6.
[0020] Specifically, the iron oxide is 120 ...
Embodiment 2
[0022] A biomass particle fuel combustion accelerant, which is composed of the following raw materials in parts by weight: 60 parts of rice husk, 35 parts of kaolin, 30 parts of diatomite powder, 3 parts of iron oxide, 6 parts of quicklime, and 11 parts of cubic stone powder.
[0023] The rice husk is specifically the rice husk dried by a dryer, and the moisture content of the rice husk is 7%.
[0024] The diatomite powder is obtained by the following method: crush the diatomite through a crusher, put the broken diatomite block into a grinder for grinding, and pass the ground diatomite powder through a 90-mesh sieve .
[0025] The above mentioned method is obtained by the following method: crushing the square stone through a crusher, putting the crushed square stone into a grinder for grinding, and passing the ground square stone powder through a 160-mesh sieve .
[0026] The plasticity of the kaolin is: strong plasticity>153.6.
[0027] Specifically, the iron oxide is 130 ...
Embodiment 3
[0029] A biomass particle fuel combustion accelerant, which is composed of the following raw materials in parts by weight: 70 parts of rice husk, 40 parts of kaolin, 40 parts of diatomite powder, 4 parts of iron oxide, 8 parts of quicklime, and 12 parts of cubic stone powder.
[0030] The rice husk is specifically the rice husk dried by a dryer, and the moisture content of the rice husk is 8%.
[0031] The diatomite powder is obtained by the following method: crush the diatomite through a crusher, put the broken diatomite block into a grinder for grinding, and pass the ground diatomite powder through a 100-mesh sieve .
[0032] The following method is obtained by the following method: crushing the cubic stone through a crusher, putting the crushed cubic stone into a grinder for grinding, and passing the ground cubic stone powder through a 170-mesh sieve .
[0033] The plasticity of the kaolin is: strong plasticity>153.6.
[0034] Specifically, the iron oxide is 140 mesh, an...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com