Ironing and shaping spray
A spray and ironing technology, which is applied in the field of clothing styling care, can solve the problems of insufficient environmental protection and styling effects, and achieve the effects of no pungent smell, simple operation in the production process, and good economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] An embodiment of the present invention provides an ironing styling spray, which is made of the following raw materials in the weight ratio: 9 parts of polyvinylpyrrolidone, 5 parts of citric acid, 3 parts of polyvinyl alcohol, and 3 parts of surfactant 7 parts of ethanol, 3 parts of essential oil, 8 parts of PEG-polydimethylsiloxane, 12 parts of glycidyl ether epoxy resin, 45 parts of carbon dioxide and 90 parts of water.
[0025] Weigh citric acid, PEG-polydimethylsiloxane and glycidyl ether epoxy resin in a magnetic stirring tank according to the formula, stir at a speed of 150r / min for 25min, stir evenly and then dry vermicelli and sieve. Add in ethanol solution for soaking to obtain a mixed solution. Put the weighed polyvinylpyrrolidone, polyvinyl alcohol, surfactant, ethanol and aromatic components into the reaction kettle to heat, and keep the heating temperature at 80°C for about 50 minutes to obtain Mixing, put the mixed liquid and the mixed material into a stir...
Embodiment 2
[0027] The ironing styling spray is made of raw materials in the following weight ratio: 10 parts of polyvinylpyrrolidone, 8 parts of citric acid, 5 parts of polyvinyl alcohol, 5 parts of surfactant, 10 parts of ethanol, 5 parts of essential oil, PEG-polymer 11 parts of dimethylsiloxane, 15 parts of glycidyl ether epoxy resin, 50 parts of nitrogen gas and 100 parts of water.
[0028] Weigh citric acid, PEG-polydimethylsiloxane and glycidyl ether epoxy resin in a magnetic stirring tank according to the formula, stir at a speed of 200r / min for 20min, stir evenly, and then dry and sieve the vermicelli. Add in ethanol solution for soaking to obtain a mixed solution. Put the weighed polyvinylpyrrolidone, polyvinyl alcohol, surfactant, ethanol and aromatic components into the reaction kettle to heat, and keep the heating temperature at 80°C for about 50 minutes to obtain Mixing, put the mixed liquid and the mixed material into a stirring tank and stir, stir well, dry, pulverize and ...
Embodiment 3
[0030] The ironing styling spray is made of raw materials in the following weight ratio: 9 parts of polyvinylpyrrolidone, 3 parts of citric acid, 3 parts of polyvinyl alcohol, 3 parts of surfactant, 6 parts of ethanol, 2 parts of essential oil, PEG-polymer 7 parts of dimethylsiloxane, 11 parts of glycidyl ether epoxy resin, 40 parts of nitrous oxide and 80 parts of water.
[0031] Weigh citric acid, PEG-polydimethylsiloxane and glycidyl ether epoxy resin in a magnetically stirred tank according to the formula, stir at a speed of 100r / min for 25min, stir evenly, dry vermicelli and sieve, Add in ethanol solution for soaking to obtain a mixed solution. Put the weighed polyvinylpyrrolidone, polyvinyl alcohol, surfactant, ethanol and aromatic components into the reaction kettle to heat, and keep the heating temperature at 80°C for about 50 minutes to obtain Mixing, put the mixed liquid and the mixed material into a stirring tank and stir, stir well, dry, pulverize and sieve to obta...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com