Connecting technology suitable for part containing complex water cooling runner of fusion reactor cladding
A technology of flow channel components and fusion reactors, which is applied in welding equipment, manufacturing tools, metal processing equipment, etc., can solve problems including deformation of complex water-cooled flow channel components, to ensure shear strength, satisfy cladding cooling effect and safety Sexual requirements, the effect of solving deformation problems
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] In this embodiment, RAFM steel is used as the water-cooling flow channel component, which is bent multiple times along the length direction and has a rectangular cross-section. A water-cooling flow channel is provided in the FAM steel along the length direction, and the cross-section of the water-cooling flow channel is square.
[0021] The joining process includes the following steps:
[0022] (1) Process the water-cooled runner components containing the above-mentioned complex water-cooled runners, and finish the surface to be welded, with a roughness lower than Ra3.2;
[0023] (2) Ultrasonic cleaning and drying of water-cooled flow channel components;
[0024] (3) After steps (1) and (2), put the water-cooled runner parts to be welded into the sheath, and the sheath is made of 304 steel;
[0025] (4) Using the vacuum electron beam welding method, the water-cooled flow channel parts to be welded are encapsulated and welded, and the vacuum leakage rate is -3 Pa m³ / S; ...
Embodiment 2
[0031] In this embodiment, 304 or 316L austenitic stainless steel is used as the water-cooling channel component, which is bent multiple times along the length direction, and the cross-section is rectangular. The 304 or 316L austenitic stainless steel is provided with a water-cooling channel along the length direction. The cross section of the channel is square.
[0032] The joining process includes the following steps:
[0033] (1) Process the water-cooled runner components containing the above-mentioned complex water-cooled runners, and finish the surface to be welded, with a roughness lower than Ra3.2;
[0034] (2) Ultrasonic cleaning and drying of water-cooled flow channel components;
[0035] (3) After steps (1) and (2), put the water-cooled runner parts to be welded into the sheath, and the sheath is made of 304 steel;
[0036] (4) Using the vacuum electron beam welding method, the water-cooled flow channel parts to be welded are encapsulated and welded, and the vacuum...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 